SAE 1020 1045 ASTM A210 St52 E355 Steel Honed Tiyo
TechniqueCold DrawnMaterialCarbon, Alloy, StainlessSurface TreatmentOiledUsageHydraulic/Otomobil Tiyo, Perçage lwil oliv/gaz, endistri machin, endistri chimik, min, objektif espesyalSection ShapeRoundProducts StandardDIN2391Steel GradeSt52,St52.3,E355,C45,AISI1020,1026,1045Tolerans StandardH6,H7,H8,H9
Voye rechèch
Chat kounye a
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Pwodwi Entwodiksyon
SAE 1020 1045 ASTM A210 St52 E355 Steel Honed Tiyo
Tablo tolerans H8
| seri ID | Tolerans | seri ID | Tolerans |
| 18< d ≤30 | +0/+0.033 | 180< d ≤250 | +0/+0.072 |
| 30< d ≤50 | +0/+0.039 | 250< d ≤300 | +0/+0.081 |
| 50< d ≤80 | +0/+0.046 | 300< d ≤315 | +0/+0.081 |
| 80< d ≤120 | +0/+0.054 | 315< d ≤400 | +0/+0.089 |
| 120< d ≤180 | +0/+0.063 | 400< d ≤500 | +0/+0.097 |

Baj popilè: sae 1020 1045 astm a210 st52 e355 asye afè tiyo, Lachin sae 1020 1045 astm a210 st52 e355 asye afine tiyo Swèd