Monel 400 Fitting tiyo
video

Monel 400 Fitting tiyo

Gnee Steel se yon byen -founisè Chinwa ki byen koni nan sektè komès etranje a, ki renome globalman pou gwo-bon jan kalite tiyo Monel 400 li yo. Gnee Steel fabrike ekipman sa yo lè l sèvi avèk alyaj prim Monel. Monel 400 se yon alyaj ki gen gwo -pèfòmans ki konpoze de kwiv ak nikèl, ki gen gwo fòs. Li montre bon rezistans alkali, rezistans asid, duktilite, ak konduktiviti tèmik, epi li ka fasil fè tèt di nan travay frèt. Alyaj sa a apwopriye pou yon pakèt aplikasyon ki soti nan -0 degre a 538 degre.
Voye rechèch
Chat kounye a

Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.

Pwodwi Entwodiksyon

 

Monel 400 Pipe Fitting deskripsyon

 

Gnee Steelse yon distribitè ki byen -koni nan sektè komès etranje a, ki renome globalman pou gwo-bon jan kalite li yo.Monel 400 tiyo fittings. Gnee Steelfabrike ekipman sa yo lè l sèvi avèk alyaj prim Monel.Monel 400se yon alyaj ki gen gwo -pèfòmans ki konpoze de kwiv ak nikèl, ki gen gwo fòs. Li montre bon rezistans alkali, rezistans asid, duktilite, ak konduktiviti tèmik, epi li ka fasil fè tèt di nan travay frèt. Alyaj sa a apwopriye pou yon pakèt aplikasyon ki soti nan -0 degre a 538 degre.

 

Monel 400 Pipe Fitting

GNEE Monel 400 Fitting tiyo

 

Fittings Monel 400 yo fèt ak yon alyaj ki gen anpil fòs -kapab reziste chaj lou ak estrès k ap travay. Pwosesis fabrikasyon an mande presyon ekstrèmman wo, sa ki lakòz fòs eksepsyonèlman wo ak fòs rupture. Li montre ekselan rezistans fatig. Menm ak ekspoze kontinyèl nan asid danjere ak konpoze, li pa fè eksperyans mete oswa korozyon. Li posede gwo rezistans nan korozyon fant, twou, ak deformation sifas yo. Monel 400 fabrike lè l sèvi avèk yon pwosesis solisyon solid, ki enplike tretman chalè ak rkwir rapid.

 

Fittings Monel 400 yo gen yon gwo pwen k ap fonn, sa ki pèmèt yo fonksyone nan anviwònman tanperati ki wo-. Yo kenbe bon pèfòmans nan aplikasyon maren epi yo rezistan a oksidasyon. Anplis de sa, ekipman sa yo lajman itilize nan jenerasyon pouvwa, pwosesis lwil oliv ak gaz, ak echanjeur chalè. Yo menm tou yo posede bon fòmabilite.

 

Nan Gnee Steel, nou ofri bon jan kalite-monel 400 Fitting nan divès gwosè ak epesè, epi nou bay koupe koutim, tretman sifas, ak sèvis livrezon mondyal pou satisfè bezwen espesifik pwojè ou yo.

Kontakte kounye a

Monel 400 Elbow
Monel 400 Reducer
Monel 400 Stub End

 

Monel 400 tiyo Fitting Spesifikasyon

 

Dimansyon ASME B16.28, MSS-SP-43, ASME/ANSI B16.9, BS4504, BS10, BS4504, BS1560,
Epesè SCH10, SCH 80, SCH 100, SCH20, SCH30, STD SCH40, SCH 160, XXS, SCH60, XS, SCH 120, SCH 140, disponib ak NACE MR 01-75
Kalite DN15-DN1200
Koneksyon Soude
Reyon koube R=2D, 3D, 5D, 6D, 8D, 1D, 10D oswa Custom
Pwosesis fabrikasyon Peze, Forge, Pouse, Jete, elatriye.
Manifakti espesyalize nan Tees, kwa, redukteur, koud 90º, fen souch, koube tiyo, koud 45º, bouchon tiyo

 

Monel 400 Fitting tiyo Spesifikasyon

 

Alloy 400 tiyo Fitting Klas ekivalan

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Monel 400 2.4360 N04400 NW 4400 NA 13 МНЖМц 28-2,5-1,5 NU-30M NiCu30Fe

 

Monel 400 Tiyo Fitting Chimik Konpozisyon

Klas C Mn Si Cu S Ti Ni Al Fe
Monel 400 0.3 max 2.0 max 0.5 max 28.0 – 34.0 0.02 max - 63.0 min 0.50 max 1.0 – 2.5

 

Alloy 400 Tiyo Fitting Pwopriyete Mekanik

Eleman Dansite Pwen k ap fonn Fòs rupture Fòs Sede (0.2% Offset) Elongasyon
Monel 400 8.8 g/cm3 1350 degre (2460 degre F) Psi - 80000, MPa - 550 Psi - 35000, MPa - 240 40 %

 

400 Monel Pipe Fittings Faktori Pwosesis

 

400 Monel Pipe Fittings Manufacturing Process

400 Monel Pipe Fittings Faktori Pwosesis

 

Monel 400 Fitting tiyo Fitting Teknik Done Fèy

 

Monel Metal 400 Alloy Tee Dimansyon

Monel Metal 400 Alloy Tee Dimension

NPS nan Equal Tee Daimèt deyò (OD)
nan bizote
Sant-pou-Fen
(C) Kouri (M) Priz
1/2" 21.3 25 25
3/4" 26.7 29 29
1" 33.4 38 38
1 1/4" 42.2 48 48
1 1/2" 48.3 57 57
2" 60.3 64 64
2 1/2" 73.0 76 76
3" 88.9 86 86
3 1/2" 101.6 95 95
4" 114.3 105 105
5" 141.3 124 124
6" 168.3 143 143
8" 219.1 178 178
10" 273.0 216 216
12" 323.8 254 254
14" 355.6 279 279
16" 406.4 305 305
18" 457.0 343 343
20" 508.0 381 381
22" 559.0 419 419
24" 610.0 432 432

 

Monel 400 alyaj koud dimansyon

Monel 400 Alloy Elbow Dimensions

Gwosè nòmal nan tiyo Deyò Dai Of (D) 90 degre
(Rayon long)
Sant-pou-Fen
(A)
45 degre
(Rayon long)
Sant-pou-Fen
(B)
90 degre
(3D)
Sant-pou-Fen
(A)
45 degre
(3D)
Sant-pou-Fen
(B)
1/2 21.3 38 16 – –
3/4 26.7 38 19 57 24
1 33.4 38 22 76 31
1¼ 42.2 48 25 95 39
1½ 48.3 57 29 114 47
2 60.3 76 35 152 63
2½ 73 95 44 190 79
3 88.9 114 51 229 95
3½ 101.6 133 57 267 111
4 114.3 152 64 305 127
5 141.3 190 79 381 157
6 168.3 229 95 457 189
8 219.1 305 127 610 252
10 273 381 159 762 316
12 323.8 457 190 914 378
14 355.6 533 222 1067 441
16 406.4 610 254 1219 505
18 457 686 286 1372 568
20 508 762 318 1524 632
22 559 838 343 1676 694
24 610 914 381 1829 757
26 660 991 406 1981 821
28 711 1067 438 2134 883
30 762 1143 470 2286 964
32 813 1219 502 2438 1010
34 864 1295 533 2591 1073
36 914 1372 565 2743 1135
38 965 1448 600 2896 1200
40 1016 1524 632 3048 1264
42 1067 1600 660 3200 1326
44 1118 1676 695 3353 1389
46 1168 1753 727 3505 1453
48 1219 1829 759 3658 1516

 

Monel 400 Pipe Fittings Dimansyon

Monel 400 Pipe Fittings Dimensions

Gwosè nòmal tiyo pou (NPS) Deyò Daimeter Pou (OD) Buttweld 90 Deg koud Buttweld 45 Deg koud Buttweld Retounen 180 Deg koud
(An pous)   Buttweld LR koud Buttweld SR koud Buttweld LR koud Buttweld LR koud
  (MM/milimèt) (pous/pous.) Sant pou fas
(An pous)
Sant pou fas
(An pous)
Sant pou fas
(An pous)
Reyon
(An pous)
Sant pou Sant
(An pous)
Retounen nan fas
(An pous)
1/2 21.3 0.840 1 1/2 – 5/8   2 1 7/8
3/4 26.7 1.050 1 1/8 – 7/16   2 1/4 1 11/16
1 33.4 1.315 1 1/2 1 7/8   3 2 3/16
1 1/4 42.2 1.660 1 7/8 1 1/4 1   3 3/4 2 3/4
1 1/2 48.3 1.900 2 1/4 1 1/2 1 1/8 3 4 1/2 3 1/4
2 60.3 2.375 3 2 1 3/8 4 6 4 3/16
2 1/2 73.0 2.875 3 3/4 2 1/2 1 3/4 5 7 1/2 5 3/16
3 88.9 3.500 4 1/2 3 2 6 9 6 1/4
3 1/2 101.6 4.000 5 1/4 3 1/2 2 1/4 7 10 1/2 7 1/4
4 114.3 4.500 6 4 2 1/2 8 12 8 1/4
5 141.3 5.563 7 1/2 5 3 1/8 10 15 10 5/16
6 168.3 6.625 9 6 3 3/4 12 18 12 5/16
8 219.1 8.625 12 8 5 12 24 16 5/16
10 273.1 10.750 15 10 6 1/4 15 30 20 3/8
12 323.9 12.750 18 12 7 1/2 18 36 24 3/8

 

Tan livrezon pou Monel 400 Pipe Fitting varye selon kote a

 

Chanjman Pri 5% anplis
Ekspòte nan Tan livrezon
UAE 5 jou
Katar 7
Lafrans 30
Kowet 10
USA 40-60
Arabi Saoudit 7
Omàn 5
Itali 30
UK 30

 

Monel 400 Pipe Fitting yo nan stock epi yo disponib pou chajman imedya pou satisfè bezwen ijan

 

Nickel 400 Equal Tee

Nikèl 400 Egal Tee

Nickel Alloy 400 45° Long Radius Elbow

Alyaj nikèl 400 45 degre koud reyon long

Nickel 400 90° Long Radius Elbow

Nikèl 400 90 degre koud reyon long

Alloy 400 Reducers

Alloy 400 redukteur

Monel 2.4360 Concentric Reducer

Monel 2.4360 redukteur konsantrik

Monel Alloy Eccentric Reducer

Monel 400 Alloy èksantrik redukteur

Monel 400 End Cap

Monel 400 End Cap

Monel Alloy 400 Stub End

Monel Alloy 400 Stub End

Alloy 400 Straight Tees and Crosses

Alloy 400 Tees dwat ak kwa

 

Pwodwi ak sèvis yo ofri pa Gnee Steel

 

Aplikasyon Monel 400 Fitting

 

Endistri petwochimik

Endistri chimik

Endistri lwil oliv ak gaz

Endistri kaka ak papye

Endistri Power Plant

Endistri Pwosesis Manje

Endistri famasetik

Endistri Enèji

Endistri Aerospace

Industry

Packaging method for Alloy 718 Pipe Fitting

Metòd anbalaj pou Alloy 400 Fitting

 

Gnee Steel itilize metòd anbalaj ki pi an sekirite ak pi efikas pou tout kalite transpò kago. Metòd anbalaj nou yo enkli:

Kès an bwa
Palettes an bwa
Retresi anbalaj anbalaj
Bwat katon
Kès an bwa (planch)

 

Alloy 400 Fittings tiyo lis pri

 

Lis pri Monel 400 Fittings tiyo Alloy 400 tiyo Fittings pri nan peyi Zend (INR) Monel Alloy 400 Pipe Fittings Pri nan USD Monel 400 Pipe Fittings Pri nan UAE (Dirham)
Pri Monel 400 90 Deg Elbow ₹ 1742 $ 36.78 USD 75.30 AED
Nikèl Alloy 400 Larsen pri pou chak Kg ₹ 484 $ 4.85 USD 24.50 AED
Monel Alloy 400 Pipe Fittings Lis Pri ₹ 2420 $ 22.21 USD 132.27 AED
Monel 400 Elbow Pri ₹ 421 $ 4.85 USD 26.50 AED
Monel 400 45 Degre Koud Pri ₹ 5204 $ 65.17 USD 256.30 AED
400 Monel Weld Fittings Pri ₹ 1257 $ 14.00 USD 64.44 AED
Lis pri Monel 400 Elbow ₹ 931 $ 17.33 USD 49.61 AED
Monel 400 Bend Price ₹ 1324 $ 14.82 USD 54.11 AED

 

Konsènan Gnee Steel

 

 

 

Konsènan Gnee Steel

Mande dènye aMonel 400 Fittinglis pri. Tanpri rele+8615824687445oswa imèlss@gneesteel.compou enfòmasyon sou stock disponib ak dènye lis pri pouNikèl 400 Fitting.

modular-1
Tanpri kontakte nou pou jwenn yon sitasyon rapid pou Monel 400 Fitting ou bezwen an

Nou bay sa yo Monel 400 Fitting ak tib dapre DIN, ISO, JIS, oswa ANSI / ASME estanda.

FAQ

K: Ki aplikasyon tiyo Monel 400 yo?

A: Akòz ekselan rezistans korozyon nan ekipman tiyo Monel 400, aplikasyon yo nan divès anviwònman korozivite yo ki nan lis anba a:

Pou egzanp, yo lajman ki itilize nan endistri pharmaceutique la.

Echanjeur chalè anjeneral itilize Monel 400 redukteur konsantrik.

Ekipman anviwònman dlo lanmè yo mande tou ekipman tiyo Monel 400.

Nikèl 400 redukteur inik yo itilize nan endistri sa yo: perçage lwil oliv lanmè, pwosesis gaz natirèl, ak jenerasyon pouvwa.

K: Ki espesifikasyon ak estanda ekipman tiyo Monel 400 yo respekte?

A: Espesifikasyon yo pou Monel 400 tiyo kout yo se ASTM B 366/ASME SB 366.

Anplis de sa, ASME/ANSI B16.9, ASME B16.28, ak MSS SP 43 yo tou estanda pou sa a kalite tiyo Fitting. Estanda sa yo kouvri tès, evalyasyon, tolerans, ak dimansyon pou ekipman tiyo ak gwosè nominal soti nan NPS ½ rive nan NPS 48.

K: Ki kondisyon yo D' pou ekipman tiyo Monel 400 nan anviwònman tanperati ki wo ak ba?

A: Nan anviwònman tanperati ki wo -, li nesesè seleksyon tanperati egzak. Idealman, ranje tanperati tipik la se ant 1200-21500 degre F.

Nan lòt men an, nan anviwònman ki ba -tanperati, nou bezwen sèvi ak materyèl douser pou amelyore lis sifas machin lan.

Baj popilè: monel 400 tiyo Fitting, Lachin monel 400 tiyo Fitting Swèd

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch