Monel 400 Bar
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Monel 400 Bar deskripsyon
Gnee Steelse yon dirijan Chinwa manifakti ak founisè nanMonel 400 ba wonn alyaj, ofri divès klas, kalite, ak gwosè. Ki baze sou diferans konpozisyon, ba wonn alyaj Monel yo klase nan plizyè klas,ki gen ladan 400, 450, ak 500, yo chak ak diferan pwopriyete mekanik.Monel alyaj 400 ba wonnyo pri pi ba pase lòt klas epi yo se youn nan pi lajman itilize yoKlas alyaj Monel. Anplis de sa, nou ofri tou ba wonn nan divès fòm, ki gen ladan wonn, egzagonal, kare, ak rektangilè, pou satisfè kondisyon aplikasyon divès.

GNEE Monel 400 Bar
Monel 400 ba yo se yon nikèl -alyaj kwiv ak yon kontni nikèl nan omwen 63% ak yon kontni kwiv nan 28-34%. Monel 400 ba ak fil montre ekselan rezistans korozyon nan yon varyete anviwònman, ki gen ladan dlo lanmè, asid, alkali, ak lòt medya korozivite. Yo menm tou yo posede gwo fòs ak bon duktilite, ki fè yo ideyal pou aplikasyon ki mande severite trè wo ak rezistans.
Akòz rezistans siperyè yo nan korozyon dlo lanmè, ba Monel 400 yo souvan itilize nan jaden jeni maren tankou konstriksyon bato, platfòm lwil oliv lanmè, ak enstalasyon bò lanmè. Yo tou yo itilize nan ekipman nan endistri chimik ki mande pou rezistans nan pwodui chimik korozivite.
Nan Gnee Steel, nou ofri bon jan kalite-monel 400 Bar nan divès gwosè ak epesè, epi nou bay koupe koutim, tretman sifas, ak sèvis livrezon mondyal pou satisfè bezwen espesifik pwojè ou yo.



Monel 400 Bar Spesifikasyon
| Bar Creole | ASTM B164 / ASME SB164 |
| Egzagòn Bar Size | 2-100mm A/F |
| Gwosè Bar wonn | Dyamèt: 3-~800mm |
| Flat Bar Size | Epesè: 2 -100mm |
| Lajè: 10 a 500mm | |
| Angle Bar Size | 3mm * 20mm * 20mm ~ 12mm * 100mm * 100mm |
| Gwosè Bar kare | 4 a 100mm |
| Chanèl Bar | 80 x 40mm a 150 x 75mm seksyon; 5.0 a 6.0mm epesè |
| Rektangilè Ba Seksyon | 3.0 a 12.0mm epesè |
| Threaded Bar Billet Size | 1/2 a 495mm Dyamèt |
| Gwosè rektang | 33 x 30mm a 295 x 1066mm |
| Hollow Bar | 32mm OD x 16mm ID a 250mm OD x 200mm ID) |
| Tolerans | H8, H9, H10, H11, H12, H13K9, K10, K11, K12 oswa selon kondisyon kliyan yo |
| Fòm | Baton, Wonn, Chanèl Bar, T-Bar, Plat Bar, Precision Ground Bar, Blòk, Kare, Bag, Round Rod, Triyang, Hollow, Rektang, Threaded, Hex (A/F), Des, Mwatye Bar, Ingot, Billet, I/H Bar, Forge elatriye. |
Monel 400 Bar Spesifikasyon
AMS 4675, AMS 4730, AMS 4731 Monel 400 Bar Ekivalan
| STANDARD | WERKSTOFF NR. | UNS | GOST | AFNOR | JIS | BS | EN |
|---|---|---|---|---|---|---|---|
| Monel 400 | 2.4360 | N04400 | МНЖМц 28-2,5-1,5 | NU-30M | NW 4400 | NA 13 | NiCu30Fe |
ASTM B164 UNS N04400 baton ak ba konpozisyon chimik
| Klas | Ni | Fe | C | Mn | Si | Cu | Al | S |
|---|---|---|---|---|---|---|---|---|
| Monel 400 | 63.0 min | 1.0 – 2.5 | 0.3 max | 2.0 max | 0.5 max | 28.0 – 34.0 | 0.50 max | 0.02 max |
Nikèl alyaj 400 baton mekanik ak pwopriyete fizik
| Dansite | Pwen k ap fonn | Fòs rupture | Fòs Sede (0.2% Offset) | Elongasyon |
|---|---|---|---|---|
| 8.8 g/cm3 | 1350 degre (2460 degre F) | Psi - 80000, MPa - 550 | Psi - 35000, MPa - 240 | 40 % |
Monel 400 Bar Pwosesis Faktori

Monel 400 Bar Pwosesis Faktori
Monel 400 Bar Fich Done Teknik
| Gwosè & dimansyon nan ba wonn Monel 400 | |||||||
|---|---|---|---|---|---|---|---|
| Metrik | US Bar | ASTM / Kanadyen | Japonè | ||||
| Gwosè Bar | Diam. (mm) | Gwosè Bar | Diam. (pous) | Gwosè Bar | Diam. (mm2) | Gwosè Bar | Diam. (mm) |
| 5 | 5 | #2 | 0.250 | 10M | 100 | 6 | 6 |
| 5.5 | 5.5 | #3 | 0.375 | 15M | 200 | 10 | 10 |
| 6 | 6 | #4 | 0.500 | 20M | 300 | 13 | 13 |
| 7 | 7 | #5 | 0.600 | 25M | 500 | 16 | 16 |
| 8 | 8 | #6 | 0.750 | 30M | 700 | 19 | 19 |
| 9 | 9 | #7 | 0.875 | 35M | 1000 | 22 | 22 |
| 10 | 10 | #8 | 1.000 | 45M | 1500 | 25 | 25 |
| 11 | 11 | #9 | 1.125 | 55M | 2500 | 29 | 29 |
| 12 | 12 | #10 | 1.250 | 32 | 32 | ||
| 14 | 14 | #11 | 1.375 | 35 | 35 | ||
| 16 | 16 | #12 | 1.500 | 38 | 38 | ||
| 18 | 18 | #13 | 1.600 | 41 | 41 | ||
| 20 | 20 | #14 | 1.750 | 44 | 44 | ||
| 22 | 22 | #15 | 1.875 | 48 | 48 | ||
| 25 | 25 | #16 | 2.000 | 51 | 51 | ||
| 28 | 28 | #18 | 2.250 | 57 | 57 | ||
| 32 | 32 | ||||||
| 36 | 36 | ||||||
| 40 | 40 | ||||||
| 44 | 44 | ||||||
| 50 | 50 | ||||||
400 pwa bar wonn monel
| Bar wonn | ||||||||
|---|---|---|---|---|---|---|---|---|
| Gwosè | Kgs / Pye | Kgs / Mtr | Gwosè | Kgs / Pye | Kgs / Mtr | Gwosè | Kgs / Pye | Kgs / Mtr |
| 3mm | 0.017 | 0.055 | 20mm | 0.753 | 2.470 | 3″ | 10.900 | 35.762 |
| 1/8″ | 0.019 | 0.062 | 22mm | 0.908 | 2.979 | 3-1/4″ | 12.800 | 41.996 |
| 5/32″ | 0.029 | 0.095 | 7/8″ | 0.926 | 3.038 | 3-1/2″ | 14.850 | 48.772 |
| 4mm | 0.030 | 0.098 | 24mm | 1.080 | 3.543 | 3-3/4″ | 17.001 | 55.780 |
| 3/16″ | 0.043 | 0.141 | 25mm | 1.180 | 3.871 | 4″ | 19.306 | 63.340 |
| 5mm | 0.047 | 0.154 | 1″ | 1.210 | 3.970 | 4-1/4″ | 21.908 | 72.249 |
| 7/32″ | 0.058 | 0.190 | 26mm | 1.271 | 4.170 | 4-1/2″ | 24.4487 | 80.340 |
| 6mm | 0.068 | 0.223 | 27mm | 1.368 | 4.490 | 4-3/4″ | 27.366 | 90.249 |
| 1/4″ | 0.076 | 0.249 | 1-1/8″ | 1.534 | 5.033 | 5″ | 30.461 | 99.940 |
| 7mm | 0.091 | 0.298 | 30mm | 1.691 | 5.548 | 5-1/2″ | 36.690 | 121.000 |
| 5/16″ | 0.118 | 0.387 | 1-1/4″ | 1.924 | 6.349 | 6″ | 43.860 | 143.900 |
| 8mm | 0.120 | 0.398 | 32mm | 1.894 | 6.314 | 6-1/2″ | 51.093 | 167.630 |
| 9mm | 0.152 | 0.498 | 1-3/8″ | 2.303 | 7.550 | 7″ | 59.432 | 196.000 |
| 3/8″ | 0.170 | 0.557 | 35mm | 2.390 | 7.553 | 7-1/2″ | 68.226 | 225.000 |
| 10mm | 0.189 | 0.620 | 36mm | 2.438 | 7.999 | 8″ | 77.586 | 254.55 |
| 11mm | 0.228 | 0.748 | 38mm | 2.792 | 8.903 | 10″ | 121.048 | 397.140 |
| Tolerans pou Cold Drawn Monel 400 Round Bar | ||
|---|---|---|
| Fòm / Seksyon | Gwosè, dyamèt oswa lajè atravè plat | Varyasyon otorize |
| mm | mm | |
| Round | Pi gran pase oswa egal a 6 Mwens pase oswa egal a 18 >18 Pi piti oswa egal a 30 >30 Mwens pase oswa egal a 50 >50 Mwens pase oswa egal a 80 >80 Mwens pase oswa egal a 100 |
+ 0 rive – 0.070 + 0 rive – 0.085 + 0 rive – 0.100 + 0 rive – 0.120 + 0 rive – 0.140 |
| Flat (epesè) | < 18 >18 Pi piti oswa egal a 30 >30 Mwens pase oswa egal a 50 >50 Mwens pase oswa egal a 80 |
+ 0 rive – 0.110 + 0 rive – 0.130 + 0 rive – 0.250 + 0 rive – 0.350 |
| Plat (lajè) | < 18 >18 Pi piti oswa egal a 30 >30 Mwens pase oswa egal a 50 >50 Mwens pase oswa egal a 80 >80 Mwens pase oswa egal a 100 >100 Mwens pase oswa egal a 130 >130 Mwens pase oswa egal a 160 >160 Mwens pase oswa egal a 320 |
+ 0 rive – 0.110 + 0 rive – 0.130 + 0 rive – 0.160 + 0 rive – 0.190 + 0 rive – 0.220 + 0 rive – 0.350 + 0 rive – 1.00 + 1.00 rive – 1.00 |
| Kare ak egzagòn |
Pi gran pase oswa egal a 6 Mwens pase oswa egal a 18 >18 Pi piti oswa egal a 30 >30 Mwens pase oswa egal a 50 >50 Mwens pase oswa egal a 80 >80 Mwens oswa egal a 105 |
+ 0 rive – 0.090 + 0 rive – 0.110 + 0 rive – 0.130 + 0 rive – 0.160 + 0 rive – 0.250 |
Tan livrezon pou Monel 400 Bar varye selon kote a
| Chanjman Pri 5% anplis | |
|---|---|
| Ekspòte nan | Tan livrezon |
| UAE | 5 jou |
| Katar | 7 |
| Lafrans | 30 |
| Kowet | 10 |
| USA | 40-60 |
| Arabi Saoudit | 7 |
| Omàn | 5 |
| Itali | 30 |
| UK | 30 |
Monel 400 Bar yo nan stock epi yo disponib pou chajman imedya pou satisfè bezwen ijan

Monel 400 Square Bar

Nikèl Alloy 400 rektangilè Bar

Nicorros LC Bright Bar

Monel 400 tè ak woule poli bar

WNR 2.4360 Kale Ba wonn

Alloy 400 Poli Bar

Monel 400 Rod

Nikèl Alloy 400 Flat Bar

ASTM B164 UNS N04400 Hex Bar
Pwodwi ak sèvis yo ofri pa Gnee Steel
Aplikasyon Monel 400 Bar
Endistri petwochimik
Endistri chimik
Endistri lwil oliv ak gaz
Endistri kaka ak papye
Endistri Power Plant
Endistri Pwosesis Manje
Endistri famasetik
Endistri Enèji
Endistri Aerospace


Metòd anbalaj pou Monel 400 Bar
Gnee Steel itilize metòd anbalaj ki pi an sekirite ak pi efikas pou tout kalite transpò kago. Metòd anbalaj nou yo enkli:
Kès an bwa
Palettes an bwa
Retresi anbalaj anbalaj
Bwat katon
Kès an bwa (planch)
Lis pri Monel 400 Bar
| Lis pri Monel 400 Bar ak fil | Alloy 400 Round Bar Pri nan peyi Zend (INR) | Monel Alloy 400 Bar ak pri fil nan USD | Nikèl alyaj 400 ba ak pri fil nan UAE (Dirham) |
|---|---|---|---|
| Pri Alloy 400 Fil | ₹ 355 | $ 4.69 USD | 16.22 AED |
| Monel Alloy 400 Fil Pri nan peyi Zend | ₹ 388 | $ 4.33 USD | 34.60 AED |
| Monel 400 Rod Pri Pa Kg | ₹ 147 | $ 5.49 USD | 4.16 AED |
| Monel 400 Rod Pri pou chak Kg nan peyi Zend | ₹ 165 | $ 4.31 USD | 6.48 AED |
| Pri nan Monel 400 Round Bar | ₹ 497 | $ 4.96 USD | 25.87 AED |
| Monel® Alloy 400 Round Bar Pri Pa Kg | ₹ 125 | $ 5.21 USD | 5.13 AED |
| Nikèl Alloy 400 Hex Bar Pri | ₹ 758 | $ 4.73 USD | 33.74 AED |
| 400 Monel Square Bar Pri | ₹ 1,159 | $ 16.75 USD | 52.50 AED |
Konsènan Gnee Steel

Mande dènye aMonel 400 Barlis pri. Tanpri rele+8615824687445oswa imèlss@gneesteel.compou enfòmasyon sou stock disponib ak dènye lis pri pouNikèl 400 Bar.

Tanpri kontakte nou pou jwenn yon sitasyon rapid pou Monel 400 Bar ou bezwen an
Nou bay sa yo Monel 400 Bar ak tib dapre DIN, ISO, JIS, oswa ANSI / ASME estanda.
FAQ
K: Ki pwa Monel 400 ba stock?
A: 7.94 liv
K: Ki sa ki dite nan stock bar kare Monel 400?
A: dite (HRc):<20
Dite (HRb): 85/90
K: Ki jan rezistans korozyon nan stock ba klere Monel 400?
A: bon rezistans korozyon
Baj popilè: monel 400 bar, Lachin monel 400 ba Swèd
Pwochen
Monel 400 Fitting tiyoOu ka renmen tou
Voye rechèch