Monel 411 N05502 Alloy Tiyo ak Tib
Monel 411 se yon alyaj nikèl-kwiv ki tipikman gen apeprè 29% kwiv ak apeprè 1.4% fè.
Voye rechèch
Chat kounye a
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Pwodwi Entwodiksyon
Monel 411 N05502 Tiyo alyaj
AMS 4677
Monel 502jido
Monel 411 N05502 Spesifikasyon tiyo alyaj
|
C |
Ni |
Taks |
Fe |
al |
Tibèkil |
Mn |
sizo |
S |
|
Mwens pase oswa egal a 0.1 |
63.0-70.0 |
balans |
Mwens pase oswa egal a 2.0 |
2.5-3.5 |
Mwens pase oswa egal a 0.5 |
Mwens pase oswa egal a 1.5 |
Mwens pase oswa egal a 0.5 |
Mwens pase oswa egal a 0.01 |