Steel rektangilè Bar SAE 8620 A+C AISI 8620 DIN 10278 DIN 1.6523 Alloy Steel Round Bar
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Steel rektangilè ba SAE 8620 A+C AISI 8620 DIN 10278 DIN 1.6523 Alloy Steel Round Bar
Deskripsyon
| Kondisyon: | Tretman Chalè | Klas asye: | Alyaj Asye |
|---|---|---|---|
| Alyaj oswa pa: | Èske alyaj | Teknik: | Woule cho, fòje, trase frèt |
| Aplikasyon: | Bar Steel estriktirèl, Bar Steel Zouti, chimik | Estanda: | ASTM, DIN, AISI, JIS |
| Fòm: | Wonn | Tretman Sifas: | Nwa / Peeling / Polisaj / Machin |
| Dyamèt: | 12mm-650mm | Dimansyon: | 5-900MM |
| Tretman chalè: | Nòmalize +Annealed +Quenched + Tanpered |
SAE {{0}} defini kòm asye alyaj ki ba kabòn ki gen 0.5% Cr, {0.2% Mo ak 0.5% Ni kòm eleman alyaj ranfòse.Li jeneralman apwovizyone kòm kondisyon rkwit ak dite HB255max.
SAE 8620 gen bon rezistans mete ak ka dite HRC 60-63 lè karburize, fè tèt di ak tanperaman. Konpare ak klas 8615 ak 8617, li montre bon fòs debaz ak pwopriyete severite ak yon seri fòs rupture tipik 700-1100 MPa, nan seksyon ti ak mwayen gwosè.
SAE 8620 apwopriye pou aplikasyon ki mande pou yon konbinezon solid ak rezistans mete. li se souvan itilize nan endistri jeni ak otomobil pou zouti ak lòt konpozan sa yo.
Aplikasyon tipik: Arbors, pignon, touf, camshafts, kingpins, ratchets, angrenaj, arbr splined elatriye.
SAE 8620 FÒM PWOVINISMAN STEEL AK GWO ak TOLERANS
| Fòm Pwovizyon pou | Gwosè (mm) | Pwosesis | Tolerans | |
| Wonn | Φ6-Φ100 | Fwad trase | Klere/Nwa | Pi bon H11 |
| Φ16-Φ350 | Woule cho | Nwa | -0{{1{1}mm | |
| Kale/tè | Pi bon H11 | |||
| Φ90-Φ1000 | Cho fòje | Nwa | -0{{1{1}mm | |
| Ki graj vire | -0{{1{1}mm | |||
| Flat/Kare/Blòk | Epesè:120-800 | Cho fòje | Nwa | -0{{1{1}mm |
| Lajè:120-1500 | Ki graj Machin | -0/+3mm | ||
Remak: tolerans ka Customized selon demann
SAE 8620 KONPOZISYON CHIMIK STEEL PA ASTM A29
| KLAS | C | sizo | Mn | P | S | Kr | Mouvman | Ni |
| 8620 | 0.18-0.23 | 0.15-0.35 | 0.70-0.90 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.040 | 0.40-0.60 | 0.15-0.25 | 0.40-0.70 |
SAE 8620 PWOPRIYETE FIZIK STEEL
| Dansite g/cm3 | 7.85 |
| Pwen fizyon Deg F | 2600 |
| Rapò Poisson a | 0.27-0.30 |
| Machinability (AISI 1212 kòm 100% machinability) | 65% |
| Ekspansyon tèmik (20 ºC) (ºC ˉ ¹) | 12.2*10^-6 |
| Kapasite chalè espesifik J/(kg*K) | 477 |
| Kondiktif tèmik W/(m*K) | 46.6 |
| Rezistans elektrik Ohm * m | 2.34*10^-7 |
SAE 8620 PWOPRIYETE MECHANIK STEEL
Pwopriyete mekanik tipik pou nwayo - carbure ak lwil oliv trempe nan 840 degre
| Gwosè Seksyon | 11mm | 30mm | 63mm |
| Fòs Tensile Mpa | 980-1270 | 780-1080 | 690-930 |
| Sede Fòs Mpa | Pi gran pase oswa egal a 785 | Pi gran pase oswa egal a 590 | Pi gran pase oswa egal a 490 |
| % elongasyon | Pi gran pase oswa egal a 9 | Pi gran pase oswa egal a 10 | Pi gran pase oswa egal a 11 |
| Charpy Enpak J | Pi gran pase oswa egal a 41 | Pi gran pase oswa egal a 41 | Pi gran pase oswa egal a 41 |
| Dite HB | 290-375 | 235-320 | 205-275 |
| Dite HRC | 31-41 | 23-35 | 16-29 |
SAE 8620 LIMIT STEEL HARDENABILITY
| Distans soti nan fen mm | 1.5 | 3 | 5 | 7 | 9 | 11 | 13 | 15 | 20 | 25 | 30 | 35 | 40 |
| HRC Min | 41 | 37 | 31 | 25 | 21 | – | – | – | – | – | – | – | – |
| HRC Max | 48 | 47 | 43 | 39 | 35 | 32 | 30 | 29 | 26 | 24 | 23 | 23 | 23 |
Valè dite anba 20HRC pa espesifye.
SAE 8620 STEEL FORGE
Tanperati Forge yo ta dwe fèt ant 925 degre -1230 degre, AISI 8620 gen kontni kabòn ki ba ki gen mwens sansib a fann pase asye kabòn mwayen oswa segondè, kidonk li ka chofe ak refwadi pi rapid. tan nan tanperati Forge yo ta dwe pi kout ke posib pou fè pou evite dekale lou ak kwasans grenn twòp. Plis pi ba tanperati a Forge ki fini, pi rafine gwosè grenn lan. Pa fòje anba tanperati minimòm Forge 850 degre.Alyaj sa a ta dwe refwadi nan. sab.
SAE 8620 STEEL NORMALIZING
Nòmalizasyon yo itilize pou rafine estrikti forgings ki ta ka refwadi ki pa inifòm apre yo fin fòje, epi konsidere kòm yon tretman kondisyone anvan ka redi. Tanperati nòmalizasyon pou asye AISI 8620 yo ta dwe fèt ant 900 degre {{3} } degre. kenbe tan apwopriye pou asye a yo dwe byen chofe ranpli ferit la nan transfòmasyon austenite. Cool nan lè toujou. Tretman sa a konsidere kòm yon lòt metòd pou amelyore machinability.
SAE 8620 RECUIT STEEL
Recuit total rekòmande pou AISI 8620 anvan D', AISI 8620 ta dwe pote nou nan yon nominale tanperati 820 degre -850 degre, kenbe apwopriye tan pou fe a byen chofe, lè sa a. refwadisman founo.
SAE 8620 KA REDI
Apre raffinage debaz, chofe tanperati a a 780oC – 820oC, kenbe tan apwopriye pou asye a yo dwe byen chofe, ak pasè nan lwil oliv.Tanperaman pi vit ke posib apre etenn.
SAE 8620 TREMPING ASYE
Tanperaman anjeneral te pote soti nan soulaje estrès nan pwosesis la redi, li pral amelyore severite a nan tou de ka ak nwayo, ak sèlman yon ti kras rediksyon nan fòs debaz ak ka dite. Chofe AISI 8620 asye a 150.oC – 200oC jan sa nesesè, kenbe ase tan jiskaske tanperati a inifòm nan tout seksyon an, tranpe pou 1 - 2 èdtan pou chak 25 mm nan seksyon, epi fre nan yon lè trankil.
SAE 8620 CABURIZING ASYE
Pake, sèl oswa gaz karburize nan tanperati 900oC – 925oC, kenbe ase tan pou jwenn pwofondè ka obligatwa a ak kontni kabòn, ki te swiv pa yon sik redi ak tanperaman apwopriye pou optimize ka ak pwopriyete debaz.
SÈTIFIKA AK TÈS TWAZI PATI
SAE 8620 Rapò MTC
Rapò tès TUV


Baj popilè: asye rektangilè bar sae 8620 a+c aisi 8620 din 10278 din 1.6523 alyaj asye wonn bar, Lachin asye rektangilè bar sae 8620 a+c aisi 8620 din 10278 din 1.6523 alyaj asye wonn ba founisè