SAE1020 ASTM Frèt Bright Bar Bar Ss400 A36 S45c Sae{{4}CrMo
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
SAE1020 ASTM Frèt Bright Bar Bar Ss400 A36 S45c Sae{{4}CrMo
Deskripsyon
| Klas asye: | Ss400 A36 S45c Sae1045 42CrMo | Alyaj oswa pa: | Ki pa Peye-alyaj |
|---|---|---|---|
| Teknik: | Cho woule, frèt trase | Aplikasyon: | Bar Steel estriktirèl |
| Kalite: | Kabòn Steel Bar | Estanda: | ASTM, DIN, AISI, JIS |
| Fòm: | Round | Longè: | 1--12m |
| Sifas: | Nwa oswa klere | Dyamèt: | 12mm{{1}m |
| Limyè segondè: |
fòje asye ba wonn,klere asye wonn ba |
||
Fwad Drawn SAE1020 Round Bar ASTM A36 Fwad Drawn Bright Round Bar
1045 trempe & apeze qt asye ba
1045 se yon asye kabòn mwayen pou jeni mekanik ak manifakti konpozan otomobil. Li ka jwenn gwo fòs ak dite segondè apre etenn ak tanperaman. Materyèl menm jan an gen ladan C43, C44, C45E, CK45, SAE1045, 080A42, S45C ETC.
Trempe ak tanperaman, abreje kòm Q & T se yon wa nan pwosesis ki ranfòse oswa redi ba asye pa chofaj materyèl yo ak Lè sa a, refwadisman nan dlo, lwil oliv oswa lòt mwayen likid, ki rapidman chanjman an soti nan austenite nan pèrlit jwenn pwopriyete yo apwopriye pou itilizasyon divès kalite. . Materyèl yo trempe & tanperaman ba asye yo anjeneral ak kabòn soti nan 0.30% - 0.60%, li se lajman itilize kòm ba komèsan nan konpozan nan machin divès kalite.
1045 materyèl ki trempe ak apeze q&t asye ba nou bay gen ladan avantaj sa yo:
Pwopriyete mekanik konsistan
Pwopriyete mekanik gwo twou san fon (soti nan sifas rive nan sant la selon kondisyon ou)
Menm dite sou ba yo antye / Pi di ak Ogmante fòs
Pa gen frajil, tès UT / tolerans gwosè presizyon / bon dwat
Bon brutality / sèvis teknik pwofesyonèl / pri konpetitif / livrezon rapid
Spesifikasyon nan 1045 materyèl trempe ak apeze q & t ba asye nou bay:
1. 1045 asye materyèl ekivalan:
| GB | ASTM/SAE/AISI | MANJE | brase | AS /NZS1444 |
| 45# | Aisi 1045 / sae 1045 / astm 1045 | C45 CK45 | S45C | AS 1045 |
2. C45 asye konpozisyon chimik:
| Materyèl | Konpozisyon chimik % | ||||||
| C | Si | Mn | S | P | Kr | Mouvman | |
| 1045 | 0.42-0.48 | 0.15-0.35 | 0.60-0.90 | 0.035 max | 0.035 max | 0.035 max | 0.035 max |
3. 1045 QT asye mekanik pwopriyete:
| Pwopriyete mekanik | ||||
| Fòs Sede (MPa) | Fòs rupture (MPa) | Elongasyon | Rediksyon nan zòn nan | Dite |
| 830 min | min660 | 12% min | 45% 25 min | 32HRC max |
4. 1045 aplikasyon asye:
gwo fòs stud boulon, Threaded Rods, van pouvwa boulon, boulon jete lank prestress, pòs ensiste boulon jete lank, Steel Tie Rod, mare ba, baton tansyon, Tansyon Bar elatriye Arbr, arbr aks, arbr, arbr pou manch rad, arbr lineyè, ponp arbr, arbr rotor, arbr Capteur, arbr spline, arbr kondwi, arbr mandrin, arbr transmisyon, baton vis elatriye machin CNC, machin CNC presizyon elatriye broch ejector ak baton ejector.
5. Liy pwodiksyon:

6. Etablisman Pwodiksyon:

7. Enspeksyon:

8. Pake:

9. RFQ:
Q1. Èske w se yon manifakti?
A1: Wi, nou gen pwòp faktori nou yo ak laboratwa pou pwodwi ak enspekte pwodwi yo.
Q2. Ki jan asire ke bon jan kalite chak pwosesis la?
A2: Depatman enspeksyon kalite nou an pral tcheke chak pwosesis ki asire bon jan kalite chak pwodwi. Nou pral pèsonèlman ale nan pwodiksyon an nan pwodwi, li faktori yo tcheke bon jan kalite a nan pwodwi yo.
Q3.Konbyen tan se tan livrezon ou a?
A3: Tan livrezon nou an se jeneralman 30 a 45 jou. Oswa selon kantite a.
Q4. Ki metòd peman ou ye?
A4:30% valè T/T an avans ak lòt 70% balans sou kopi B/L.
Q5.Èske ou ka bay yon echantiyon?
A5: Asire w, echantiyon nou an bay gratis, men li pa enkli frè courrier


Baj popilè: sae1020 astm frèt trase klere wonn bar ss400 a36 s45c sae1045 42crmo, Lachin sae1020 astm frèt trase klere wonn bar ss400 a36 s45c sae1045 42crmo founisè
Ou ka renmen tou
Voye rechèch