6m Longè ASTM A276 201 304 316L Inegal Egal L Profiles Nerjaveèi ang BarDescriptionProducts: Nerjaveèi asye ang Bar, chanèl Bar, plat Bar Klas: 201 304 316 LType: Ang Bar/Chanèl Bar / Flat Bar Longè: 6mOther Materyèl : Chanèl Bar, Flat Bar, wonn Bar.etc Size: Tout gwosè estanda nan StockDeliver Tan: Nan 10 jou Sèvis: CuttingHigh limyè: ASTM A 276 304 Nerjaveèi ang ba, 201 Nerjaveèi ang ba, 316L Nerjaveèi ang ba
Voye rechèch
Chat kounye a

Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.

Pwodwi Entwodiksyon

 

50x50 * 5mm 6000mm Sus304 Nerjaveèi asye Angle Bar

Deskripsyon

Pwodwi: Nerjaveèi asye Angle Bar Klas: 304 316L
Kalite: Ang Bar Longè: 6m
Lòt materyèl: Chanèl Bar, Flat Bar, wonn Bar.etc Kalite konpayi: Faktori
Livre tan: Nan 10 jou Sèvis: Koupe
Segondè limyè:

sus304 ba ang asye pur

,

50x50 sus304 asye pur ang ba

,

5mm sus304 asye pur ang ba

ASTM A276 Klas 304 Nerjaveèi asye Angle Bar / SS Angle Nerjaveèi asye / Steel Angle Iron

 

Komodite ba ang asye pur
Gwosè 20mmx20mmx3mm ~ 150mmx150mmx12mm
Longè 6m, oswa kòm Customized
Sifas woule cho
Aplikasyon Konstriksyon jaden, endistri konstriksyon bato, petwòl ak endistri chimik, endistri lagè ak elektrisite, pwosesis manje ak endistri medikal, echanj chalè chofaj, jaden pyès ki nan konpitè machin.
Tan livrezon 5 - 8 jou, selon kantite
Regleman pri FOB/ CFR% 2f CIF
Pake Ekspòte pake estanda, oswa selon kondisyon kliyan yo
Lòt Pwodwi Nerjaveèi asye chanèl ba, Nerjaveèi asye wonn ba, Nerjaveèi asye plat ba, Nerjaveèi asye egzagòn ba

 

Eleman (Wt.%)

 

  C Mn P S sizo Kr Ni N Mouvman Ti
201 0.15max 5.50-7.50 0.06max 0.030max 1.00max 16.00-18.00 3.50-5.50 0.25max - -
304 0.08max 2.00max 0.045max 0.030max 1.00max 17.50-19.50 8.00-10.50 0.10max - -
316L 0.03max 2.00max 0.045max 0.030max 1.00max 16.00-18.00 10.00-14.00 - 2.00-3.00 -


Pwopriyete mekanik

 

Atik materyèl Fòs rupture (MPa) Fòs Sede (MPa) Ekstansyon Dite (HV) Dansite
201 Pi gran pase oswa egal a 520 Pi gran pase oswa egal a 275 Pi gran pase oswa egal a 40% <253 7.93g/cm³
304 Pi gran pase oswa egal a 520 Pi gran pase oswa egal a 205 Pi gran pase oswa egal a 40% Mwens pase oswa egal a 200 7.93g/cm³
316L Pi gran pase oswa egal a 480 Pi gran pase oswa egal a 177 Pi gran pase oswa egal a 40% Mwens pase oswa egal a 200 7.98g/cm³

 

Enfòmasyon detaye pwodwi nou yo

 

Nerjaveèi asye ang ba

Klas:201 304 316L 310S.etc

Gwosè: 30 * 30 * 3mm -150 * 150 * 10mm x 6m longè

Kalite: ang egal

Nerjaveèi asye chanèl ba

Klas:201 304 316L 310S.etc

Gwosè:4# - 20#

Kalite: U channel

Nerjaveèi asye wonn ba

Klas:201 304 316L 310S 321 2205 2507 904L.etc

Gwosè:4 - 350mm

Kalite: ba nwa, ba klere

Nerjaveèi asye egzagòn ba

Klas:201 304 316L 410 420 430.etc

Gwosè: 5x5 - 60 x 60

Kalite: frèt trase

Nerjaveèi asye plat ba

Klas:201 304 316L 310S 2205 2507 321 904L 410 420 430.etc

Gwosè: 10 * 3 - 200 * 50mm

Kalite: woule cho

 

 

 

50x50*5mm 6000mm Sus304 Stainless Steel Angle Bar 050x50*5mm 6000mm Sus304 Stainless Steel Angle Bar 150x50*5mm 6000mm Sus304 Stainless Steel Angle Bar 2

Baj popilè: 6m longè astm a276 201 304 316l inegal egal l pwofil asye pur ang ba, Lachin 6m longè astm a276 201 304 316l inegal egal l pwofil asye pur ang ba founisè

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch