Nerjaveèi asye 321/321Hse Titàn estabilize plak asye pur ak fèy ak bon pwopriyete mekanik. Plak ak fèy asye pur sa yo ofri ekselan rezistans korozyon epi yo gen ekselan rezistans nan korozyon entè-granulaire apre yo fin ekspoze li nan seri a carbure chromium nan tanperati. Yo menm tou yo gen pi wo ranpe ak pwopriyete rupture estrès konpare ak lòt alyaj. Nerjaveèi asye 321/321H plak ofri tou bon rezistans ba-tanperati ak fòs siperyè. Plak 321h sa yo itilize tou nan asid òganik dilye nan tanperati mwayen. Yo ofri tou kèk lòt karakteristik tankou gwo fòs rupture, durability, konsepsyon egzak ak sou sa.



KaliteSS 321/321H Fèy ak Plak yoke nou ofri yo se plak SS 321H woule, plak woule frèt, bobin 321/321H, bann, FOIL, fèy Shim, fèy pèse, sèk, plak poli, plak woule cho, bag, ak anpil plis.
Gen anpil aplikasyon endistriyèl kote plak asye pur sa yo ak fèy yo itilize epi yo ofri pèfòmans ekselan. Plizyè aplikasyon SS 321/321H Sheets & Plates yo se plant jenerasyon pouvwa, raffineries lwil oliv lanmè, endistri pwosesis gaz, pwodui chimik espesyal, famasetik, ekipman famasetik, ekipman chimik, echanjeur chalè, endistri pâtes ak papye, pétrochimique, ak sou sa. .
NOU bay tout sètifika tès materyèl yo an akò ak EN 20204/3.1B ak kèk nan yo se sètifika matyè premyè, 100% rapò tès radyografi, rapò enspeksyon twazyèm pati, ak sou sa. Nou menm tou nou te fè diferan tès materyèl sou pwodwi sa yo asire bon jan kalite a nan pwodwi sa yo anvan nou voye yo bay kliyan nou yo.
321/321H Fèy Nerjaveèi ak Plak KLAS EKIVILAN
| STANDARD | DEZOLE | WNR. | ANNWI | EN |
|---|---|---|---|---|
| SS 321 | S32100 | 1.4541 | SUS 321 | X6CrNiTi18-10 |
| SS 321H | S32109 | 1.4878 | SUS 321H | X12CrNiTi18-9 |
Fèy asye pur ak plak spesifikasyon:ASTM A240 / ASME SA240
Dimansyon estanda:JIS, AISI, ASTM, GB, DIN, EN, elatriye
Lajè:1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, elatriye
Longè:2000mm, 2440mm, 3000mm, 5800mm, 6000mm, elatriye
Epesè:0.3 mm rive 120 mm
Fòm:Bobin, FOIL, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Checkered Plate, Strip, Flats, Blank (Sèk), Ring (Flange) elatriye.
Fini sifas:Plak woule cho (HR), fèy woule frèt (CR), 2B, 2D, BA, NO.1, NO.4, NO.8, 8K, glas, Chequered, Relief, liy cheve, eksplozyon sab, Bwòs, grave, SATIN (Met ak plastik kouvwi) elatriye.
KONPOZISYON CHIMIK FYÈY AK PLAK EN 321/321H.
| % | Kr | Ni | C | sizo | Mn | P | S | N | Tibèkil | Fe |
|---|---|---|---|---|---|---|---|---|---|---|
| 321 | min:17.0 max:19.0 |
min: 9.0 max:12.0 |
max:0.08 | max:0.75 | max:2.0 | max:0.045 | max:0.03 | max:0.10 | min:5*(C+N) max:0.70 |
Balans |
| 321H | min:17.0 max:19.0 |
min: 9.0 max:12.0 |
min:0.04 max:0.10 |
min:18.0 max:20.0 |
max:2.0 | max:0.045 | max:0.03 | max:0.10 | min:5*(C+N) max:0.70 |
Balans |
PWOPRIYETE MEKANIK FEYÈ AK PLAK EN 321/321H.
| Klas | Fòs rupture ksi (min.) |
Sede fòs 0.2% Offset ksi (min.) |
elongasyon - % nan 50 mm (min.) |
Dite (Brinell) MAX |
|---|---|---|---|---|
| 321/321H | 75 | 30 | 40 | 217 |