EW QStE500TM asye plak/fèy Segondè fòs sede pou asye frèt fòme SEW092 QStE500TM asye plak/fèy, SEW092 QStE500TM asye plak/fèy, nou ka konsidere QStE500TM asye plak/fèy kòm asye fòs segondè sede pou asye frèt-fòme.
Voye rechèch
Chat kounye a

Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.

Pwodwi Entwodiksyon

 

SEW {{0}} QSTE500TM HR500F S500MC marinated bobin asye plak 3.0 * 1250 * 2500mm

Deskripsyon

Lajè: {{0}mm Teknik: Sou entènèt jwèt Cho woule marinated
Kalite: Steel plak, bobin asye Estanda: ASTM, AISI, JIS, DIN
Longè: {{0}mm Itilizasyon espesyal: Plak asye wo-fòs, cho woule
Epesè: 0.5-100mm Sifas: Nwa pentire
Segondè limyè:

3mm cho woule Kabòn Steel plak

,

3mm Cho woule Kabòn Steel Fèy

,

DIN cho woule kabòn Steel plak

SEW {{0}} QSTE500TM HR500F S500MC marinated bobin asye plak 3.0 * 1250 * 2500mm

 

EW QStE500TM asye plak/fèy Segondè fòs sede pou asye frèt fòme

SEW092 QStE500TM asye plak / fèy, SEW092 QStE500TM asye plak / fèy, nou ka konsidere QStE500TM asye plak / fèy kòm asye fòs segondè sede pou asye frèt-fòme.

Plak asye QStE500TM se sitou itilize kòm asye fòs segondè sede pou asye frèt-fòme.
SEW092 QStE500TM asye a ekivalan a EN S500MC, NFA E490D, UNI FeE490TM ak ASTM X70XLK klas asye.

QStE500TM SEW092 Nimewo: 1.0984 Konparezon nan klas asye
EN 10149-2 S500MC
NFA36-231 E490D
UNI8890 JIbyalite
ASTRA 070xlk
BS1449 -

QStE500TM asye Chimik Konpozisyon

Klas C max Si max Mn max P max S max AL max Nb max V max Ti max
QStE500TM 0.12 0.50 1.7 0.025 0.015 0.015 0.09 0.2 0.15

QStE500TM asye Pwopriyete mekanik

Epesè nominal (mm) -
ReH-Minimun fòs sede (Mpa) 500
Epesè nominal (mm) -
Rm-tansyon fòs (Mpa) 550-700
Epesè nominal (mm) Soti nan 3
A-Minimòm elongasyon Lo=5,65√So(%) 14
Epesè nominal (mm) pou3
A-Minimòm elongasyon Lo=Lo=80mm(%) 12

nou se founisè asye QStE500TM, tou ka bay QStE550TM asye, QStE600TM asye, QStE690TM asye, tanpri kontakte nou si ou bezwen

 

 

 

 

SEW 092-1990 QSTE500TM  HR500F S500MC  Pickled Coil Steel Plate 3.0*1250*2500mm 0SEW 092-1990 QSTE500TM  HR500F S500MC  Pickled Coil Steel Plate 3.0*1250*2500mm 1SEW 092-1990 QSTE500TM  HR500F S500MC  Pickled Coil Steel Plate 3.0*1250*2500mm 2

Baj popilè: koud {{0}} qste500tm hr500f s500mc marinated bobin asye plak 3.0 * 1250 * 2500mm, Lachin koud 092-1990 qste500tm hr500f s500mc marinated bobin asye plak 3.0 * 1050mm founisè *

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch