Segondè fòs rupture E350C asye plak S335J 2+N cho woule plak
Segondè fòs rupture E35 0C Steel plak S335J2+N Hot Rolled PlateDescriptionWidth: 600-2500mm Klas: S335J{2+NTeknik: Cho woule Kalite: Steel PlateStandard: ASTM,GB, AISI,JIS,DIN Longè: 1000-12000mmSurface Tretman: Hot Fini Itilizasyon Espesyal: High-fòs Steel PlateThickness: 0.5-100mm Zenk Kouch: Plak asye modere ka Limyè ProceHigh: Stock bobin asye pur, woule frèt bobin asye pur
Voye rechèch
Chat kounye a
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Pwodwi Entwodiksyon
Segondè fòs rupture E350C asye plak S335J 2+N cho woule plak
Deskripsyon
| Lajè: | 600-2500mm | Klas: | S335J2+N |
|---|---|---|---|
| Teknik: | Woule cho | Kalite: | Plak asye |
| Estanda: | ASTM, GB, AISI, JIS, DIN | Longè: | 1000-12000mm |
| Tretman Sifas: | Cho fini | Itilizasyon espesyal: | Plak asye wo-fòs |
| Epesè: | 0.5-100mm | Zenk kouch: | Plak asye modere ka Proce |
| Limyè segondè: |
stock bobin asye pur,woule frèt bobin asye pur |
||
Espesifikasyon estanda
Estanda
EN 10025-2:2004
Lajè
1000mm-4500mm
Epesè
3mm-150mm
Enpak teste:
-52 degre C
Longè
3000mm -18000mm
Pwosesis
Woule cho (HR)
Tès destriktif ak ki pa destriktif
Mekanik ekzamine tankou tansyon, elongasyon
ak rediksyon nan zòn nan.
Chimik egzamen-Spectro analiz
Analiz enpak
Analiz idrostatik
Rekonesans materyèl pozitif
Tès radyografi
Tès fèm
S355J2+N / E350 C Pwosesis Plak
Koupe
Fòme Perçage / Machining
Manje
Tès
S355J2+N Klas ekivalan:
| Klas | DIN | ASTM | EN | JIS | Materyèl non. |
| S355 J2+N | 17100 St52-3N |
A572-50 | 10025-2:2004 | G3106 SM490YB |
1.0577+N |
Konpozisyon chimik nan plak S355J2+N / E350 C
| Klas | C | Si | Mn | S | P | C.E |
| S355 J2+N | 0.22 max | 0.55 max | 1.60 max | 0.035 max | 0.035 max< | 0.047 max |
| (E350) Fe 490 | 0.20 max | 0.45 max | 1.50 max | 0.045 max | 0.045 max< | - |
Pwopriyete mekanik S355J2+N / E350 C Steel Plak
| Klas | Epesè (mm) | Sede fòs Rehmin (N / mm²) | Fòs rupture Rmmin (N / mm²) | Elongasyon A5 min (%) | Impact Values Charpy-V-Notch LongitudinalAverage from 3 Speimens Thk.>10<150mm. |
| S355J2+N | 3<> | 315-355 | 490-630 | maksimòm 22 | 27 Joul nan -20 C |
| E350 | <20mm->40mm | 320-350 | 490 | 22% | 25 Joul nan -20 C |


Baj popilè: segondè fòs rupture e350c asye plak s335j2+n cho woule plak, Lachin segondè fòs rupture e350c asye plak s335j2+n cho woule plak founisè