SUS304 ASTM A554 Nerjaveèi asye kare tiyo

Non atik: Nerjaveèi asye soude oswa san pwoblèm tib kare pou balistrad
Estanda: ASTM A554 oswa A312
Klas materyèl: AISI 201, 202, 304, 304L, 316, 316L, elatriye.
Sètifika: ISO 9001% 3a 2008
Dimansyon: 10 mm x 10 mm - 200 mm x 200 mm (Gade Range Anba)
Epesè mi: {{{}}}}.3 mm - 5.0 mm
Sifas: Poli 320 G, 400 G, 600 G; Cheve; Dechaje.
Longè: 10 mm - 10000 mm
Anbalaj: Chak oswa plizyè tib (tiyo) ta dwe manch nan sache plastik endividyèlman, ak Lè sa a, yon pake nan yo ta dwe chaje pa yon sak resi ki se marin.
Aplikasyon: Dekorasyon, konstriksyon ak bilding, tankou balistrad, balistrad, fenèt, mèb, elatriye.
Chimik
Konpozisyon:
Klas Materyèl C sizo Mn P S Ni Kr Mouvman
Ezi 201 Mwens pase oswa egal a 0.15 Mwens oswa egal a 1.00 5.50~7.50 Mwens pase oswa egal a 0.060 Mwens pase oswa egal a 0.03 1.00 ~1.50 13.50~15.00 \
AISI 202 Mwens pase oswa egal a 0.15 Mwens oswa egal a 1.00 7.50~10.00 Mwens pase oswa egal a 0.060 Mwens pase oswa egal a 0.03 4.00~6.00 17.00~19.00 \
AISI 304 Mwens pase oswa egal a 0.08 Mwens oswa egal a 1.00 Mwens pase oswa egal a 2.00 Mwens pase oswa egal a 0.045 Mwens pase oswa egal a 0.03 8.00~11.00 18.00~20.00 \
AISI 304L Mwens pase oswa egal a 0.035 Mwens oswa egal a 1.00 Mwens pase oswa egal a 2.00 Mwens pase oswa egal a 0.045 Mwens pase oswa egal a 0.03 8.00~13.00 18.00~20.00 \
AISI 316 Mwens pase oswa egal a 0.08 Mwens oswa egal a 1.00 Mwens pase oswa egal a 2.00 Mwens pase oswa egal a 0.045 Mwens pase oswa egal a 0.03 10.00~14.00 16.00~18.00 2.00~3.00
AISI 316L Mwens pase oswa egal a 0.035 Mwens oswa egal a 1.00 Mwens pase oswa egal a 2.00 Mwens pase oswa egal a 0.045 Mwens pase oswa egal a 0.03 10.00~14.00 16.00~18.00 2.00~3.00
Mekanik
Pwopriyete:
Klas Materyèl elongasyon (%) Tensile fòs (Rm) N/m m³ Fòs Sede (Rp) 0.2% N/m m³ Dite (HV)
AISI 201 Pi gran pase oswa egal a 35 Pi gran pase oswa egal a 520 Pi gran pase oswa egal a 210 Mwens pase oswa egal a 253
EZI 202 Pi gran pase oswa egal a 35 Pi gran pase oswa egal a 590 Pi gran pase oswa egal a 210 Mwens pase oswa egal a 218
AISI 304 Pi gran pase oswa egal a 35 Pi gran pase oswa egal a 520 Pi gran pase oswa egal a 210 Mwens pase oswa egal a 200
AISI 304L Pi gran pase oswa egal a 35 Pi gran pase oswa egal a 480 Pi gran pase oswa egal a 180 Mwens pase oswa egal a 200
AISI 316 Pi gran pase oswa egal a 35 Pi gran pase oswa egal a 520 Pi gran pase oswa egal a 210 Mwens pase oswa egal a 200
AISI 316L Pi gran pase oswa egal a 35 Pi gran pase oswa egal a 480 Pi gran pase oswa egal a 180 Mwens pase oswa egal a 200