Rektangilè Tib En 10025 S355
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Black Carbon ERW Gwo Dyamèt Rektangilè Tib En 10025 S355 100x200x6mm
Deskripsyon
| Sètifikasyon: | ISO9001-2000 | Alyaj oswa pa: | Ki pa Peye-alyaj |
|---|---|---|---|
| Teknik: | ERW | Epesè: | 2.87 - 13.84 Mm |
| Aplikasyon: | Estrikti tiyo | Longè: | 5.8-12m |
| Fòm: | Kare | ||
| Limyè segondè: |
en 10025 gwo dyamèt rektangilè tib,100x200 gwo dyamèt rektangilè tib,s355 kabòn rektangilè tib |
||
SS400 Nwa Soude Steel Tib Kare RHS 0.45 - 30 mm Epesè Mi
| GWO: | 10x10-1200x1200mm |
| GWO TORLERANS: | +/-0.03mm |
| Epesè mi: | 0.45-30mm |
| TORLERENCE: | +/-0.03mm |
| STANDARD: | GB/T 3094-2000 ASTM A 500 JIS G 3466 |
| SÈTIFIKA: | ISO BV SGS |
| MATERYÈL: | Q195 /Q215/Q235/ Q345 |
| TEKNIK: | Soude, woule frèt. |
| FÒM SEKSYON: | Rektangilè |
| Anbalaj: |
1. Nan pake ak teren 2. Pa materyèl PP tissus ak plastik anti-dlo 3. Kòm kondisyon kliyan an. |
|
SIfas TRETMAN: |
1) Nwa, Pre-galvanize 2) lwil oliv, kouch poud 3) galvanize kòm kondisyon ou |
| Itilizasyon: |
Machin-fè, fabrikasyon machin, ankadreman veso, Mèb |
| MACHE PRINCIPAL: | Mwayen Oryan, Afrik, Nò ak Amerik di Sid, Lès ak Lwès Ewòp, Azi Sidès Ostrali |
| PEMAN & KONDISYON LIBRE: | |
| KANTITE MINIMÒM LÒD: | 25 ton metrik |
| PORT: | SHANGHAI |
| TAN LIVRAISON: | 20 jou apre li fin resevwa LC a oswa depo |
| TÈM PEMAN: | LC nan je TT D/P, ect |
| KAPASITE PWOVNI: | 10000mts pa mwa |
EN 10025 S355 Steel
S355 asye se yon estanda Ewopeyen an asye estriktirèl klas, dapre EN 10025-2: 2004, materyèl S355 divize an 4 klas kalite prensipal:
S355JR (1.0045),
S355J0 (1.0553),
S355J2 (1.0577) ak
S355K2 (1.0596).
Pwopriyete estriktirèl asye S355 pi bon pase asye S235 ak S275 nan fòs sede ak fòs rupture.
Steel Klas S355 Siyifikasyon (Deziyasyon)
Lèt ak nimewo sa yo eksplike klas asye S355 siyifikasyon an.
"S" se kout pou "asye estriktirèl"
"355" refere a valè fòs sede minumum pou epesè asye plat ak long ki pi piti pase oswa egal a 16mm.
"JR" vle di valè enèji enpak la se pi piti 27 J nan tanperati chanm (20 degre).
"J{{0}}" ka kenbe tèt ak enèji enpak omwen 27 J nan 0 degre.
"J2" ki gen rapò ak valè enèji enpak minimòm lan se 27 J nan -20 degre.
"K2" vle di valè enèji enpak minimòm se 40 J nan -20 degre.
Fichye done ak spesifikasyon
Anba a se tab yo montre fichye done S355 klas asye a ki gen ladan konpozisyon chimik, fòs sede, fòs rupture ak elongasyon, elatriye. Tout fèy done DIN EN 10025-2 se menm jan ak BS EN 10025-2 ak lòt Inyon Ewopeyen an. eta manm yo.
Konpozisyon chimik
Fich done ki anba a montre konpozisyon chimik asye klas S355.
| S355 % Konpozisyon chimik (mwens pase oswa egal a) | ||||||||||
| Estanda | Steel | Klas | C | Si | Mn | P | S | Cu | N | Metòd dezoksidasyon |
| EN 10025-2 | S355 | S355JR | 0.24 | 0.55 | 1.60 | 0.035 | 0.035 | 0.55 | 0.012 | Rimmed asye pa pèmèt |
| S355J0 (S355JO) | 0.20 | 0.55 | 1.60 | 0.030 | 0.030 | 0.55 | 0.012 | |||
| S355J2 | 0.20 | 0.55 | 1.60 | 0.025 | 0.025 | 0.55 | – | Totalman touye | ||
| S355K2 | 0.20 | 0.55 | 1.60 | 0.025 | 0.025 | 0.55 | – | Totalman touye | ||
Pwopriyete mekanik
Fichye done ki anba a bay EN 10025 S355 pwopriyete mekanik asye tankou fòs sede, fòs rupture ak elongasyon.
Sede fòs
| S355 Sede Fòs (Pi gwo pase oswa egal a N/mm2); Dia. (d) mm | |||||||||
| Steel | Klas Steel (Nimewo Steel) | d Pi piti oswa egal a 16 | 16< d ≤40 | 40< d ≤63 | 63< d ≤80 | 80< d ≤100 | 100< d ≤150 | 150< d ≤200 | 200< d ≤250 |
| S355 | S355JR (1.0045) | 355 | 345 | 335 | 325 | 315 | 295 | 285 | 275 |
| S355J0 (1.0553) | |||||||||
| S355J2 (1.0577) | |||||||||
| S355K2 (1.0596) | |||||||||
Fòs rupture
| S355 Fòs Tensile (Pi gwo pase oswa egal a N/mm2) | ||||
| Steel | Steel Klas | d<3 | 3 Mwens pase oswa egal a d Mwens pase oswa egal a 100 | 100 < d Mwens pase oswa egal a 250 |
| S355 | S355JR | 510-680 | 470-630 | 450-600 |
| S355J0 (S355JO) | ||||
| S355J2 | ||||
| S355K2 | ||||
Elongasyon
| elongasyon (pi gran pase oswa egal a %); Epesè (d) mm | ||||||
| Steel | Steel Klas | 3 Mwens pase oswa egal a d Mwens pase oswa egal a 40 | 40< d ≤63 | 63< d ≤100 | 100< d ≤ 150 | 150< d ≤ 250 |
| S355 | S355JR | 22 | 21 | 20 | 18 | 17 |
| S355J0 (S355JO) | ||||||
| S355J2 | ||||||
| S355K2 | 20 | 19 | 18 | 18 | 17 | |



FAQ
K: Ki jan ou kontwole bon jan kalite?
A: Sètifikasyon Tès Mill yo apwovizyone ak chajman, Enspeksyon Twazyèm Pati ki disponib. epi nou jwenn tou ISO, SGS, alibaba verifye.
K: Ki avantaj ki genyen nan konpayi ou a?
A: Nou gen anpil pwofesyonèl, pèsonèl teknik, pri pi konpetitif ak pi bon sèvis apre-dales pase lòt konpayi asye pur.
K: Konbyen peyi ou deja ekspòte?
A: Ekspòte nan plis pase 50 peyi sitou nan Amerik, Larisi, UK, Kowet, peyi Lejip, Latiki, lòt bò larivyè Jouden, peyi Zend, elatriye.
K: Èske ou ka bay echantiyon?
A: Wi. Nou ka bay ti echantiyon yo nan stock gratis, osi lontan ke ou kontakte nou. Echantiyon Customized pral pran apeprè 5-7 jou.
Baj popilè: rektangilè tib en 10025 s355, Lachin rektangilè tib en 10025 s355 Swèd
Ou ka renmen tou
Voye rechèch