Fwad trase tiyo asye san pwoblèm presizyon tib kabòn asye DIN2391 EN10305 ST37 ST52

Fwad trase tiyo asye san pwoblèm presizyon tib kabòn asye DIN2391 EN10305 ST37 ST52

DIN2391 EN10305 ST37 ST52 Seamless Precision Carbon Steel Tube1, Estanda: ASTM / DIN / EN / GOST / SAE / JIS etc2, Klas Materyèl: Steel Steel / Alloy Steel oswa selon kondisyon.
Voye rechèch
Chat kounye a

Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.

Pwodwi Entwodiksyon

 

Fwad trase tiyo asye san pwoblèm presizyon tib kabòn asye DIN2391 EN10305 ST37 ST52

Deskripsyon

OD: 6-159MM Epesè: 0.5-10mm
Sifas: Klere Longè: 6m
Kalite: Fwad trase
Segondè limyè:

tiyo asye lou

,

tiyo asye estriktirèl

 

Fwad trase tiyo asye san pwoblèm presizyon tib kabòn asye DIN2391 EN10305 ST37 ST52

 

DIN2391 EN10305 ST37 ST52 san pwoblèm presizyon Kabòn Steel Tib

1, Estanda: ASTM / DIN / EN / GOST / SAE / JIS elatriye

2, Klas Materyèl: Kabòn Steel / Alloy Steel oswa selon kondisyon.

Gwosè: (mm)

OD: 19.05 mm

WT: 2.11 mm;

Longè: max 25m

 

 

Deskripsyon:

 

Non pwodwi: Tib echanjeur chalè / Fwad Drawn / ERW

Estanda egzekitif: ASTM / DIN / EN / GOST / SAE / JIS elatriye

(ASTM A179,ASTM A199, ASTM A200, ASTM A213, DIN 17175,JIS G3462,JIS G3458)

Dyamèt deyò: 19.05mm

Epesè miray: 2.11mm

Longè: 6m-25m, tou ka fabrike selon kondisyon kliyan yo

Kalite: trase frèt oswa ERW

Fen: pwent plen oswa pwent bizote

Kondisyon livrezon: BK, BKS, BKW, NBK, GBK (Kòm trase, trempe ak tanperaman, nòmalize, rkwit, soulaje estrès) Kòm diferan kondisyon, Li enkli marinated, elatriye. AS per Standard.

Kouch pou pwoteksyon: penti nwa, anti-rouye lwil oliv oswa vèni, tou yo ka mande selon kondisyon kliyan yo

 

 

Tès faktori ak lòt tèm:

 

1.Hydrostatic oswa Nondestructive Electric Test

2.Heat Tretman: dapre Creole
3.Sifas kondisyon: Selon Standard.
4.Grain Size:Dapre estanda
5.Sampling: plati, flare, gwosè grenn, Marking

6.nou bay fen bizo, bouchon plastik, kouch vèni, lwil oliv oswa nwa pentire pou anpeche rouye ak lòt anbalaj

sèvis.

 

 

Detay prensipal spesifikasyon:

 

Non Fwad trase oswa ERW dwat tib asye ak tiyo pou echanjeur chalè
Estanda

Satisfè oswa depase estanda ASTM, ASME, API, ANSI ak DIN.

ASTM A106/A179/A192/A210/A213/A519 elatriye.

DIN2391/DIN17175/EN10305 elatriye

GB8162/GB8163/GB3639 elatriye

Materyèl

A179% 2cSt35,St45% 2cSt52,E215,E235,E355,10,20,

A106, A179, A192, A210, T11, T22, T12 elatriye

Gwosè

Dyamèt ekstèn: {{0}}.0mm

Epesè miray la:0.5-15mm

Longè: max 2400mm, jeneralman 6000mm

Aplikasyon

Fwad trase oswa frèt woule presizyon tib asye san pwoblèm pou presyon idwolik ak

sèvis chanm konpwesyon lè.


Pou itilize oto, itilize machin, tib silenn lwil oliv, itilize redukteur chòk motosiklèt, chòk oto

redukteur silenn enteryè, elatriye.

 

Tiyo asye san pwoblèm pou chodyè presyon ki ba ak mwayen, chodyè presyon ki wo,

konstriksyon bato, sèvis likid, krak petwòl, ekipman angrè chimik,

Desen-lwil oliv-ekipman ak objektif estrikti.

Dimansyon biznis

DIN seri frèt trase presizyon tib asye san pwoblèm

DIN seri frèt woule presizyon tib asye san pwoblèm

Ki gen rapò kouvwi ak galvanised tib asye

Tib fosforil ki enpèmeyab

Prensipalkarakteristik

Pa gen kouch oksidasyon sou mi yo deyò ak enteryè;

Pa gen flit anba presyon ki wo;

Pa gen Crake anba plat ak plat;

Pa gen deformation apre koube frèt;

Segondè presizyon segondè pwòpte;

Ekselan klète

frèt trase ak cho fini

Pèfòmans siperyè pou gwo presyon ak itilizasyon tanperati

Nwa fini ak plonje cho galvanised

Ekselan rezistans korozyon

 

 

Kondisyon livrezon:

 

Deziyasyon Senbòl Deskripsyon
Fwad fini (difisil) MASK Tib pa sibi tretman chalè apre fòm final la frèt epi, kidonk, gen yon rezistans olye segondè nan deformation.
Fwad fini (mou) BKW Se tretman chalè final la ki te swiv pa desen frèt ki enplike deformation limite. Apwopriye plis pwosesis pèmèt yon sèten degre frèt fòme. (egzanp koube, agrandi).
Fwad fini ak estrès-soulaje Mask yo Se tretman chalè aplike apre dènye pwosesis la frèt fòme. Sijè a kondisyon pwosesis apwopriye, ogmantasyon nan estrès rezidyèl ki enplike pèmèt tou de fòme ak machin nan yon sèten degre.
Rkwit BASKÈTBÒL Dènye pwosesis frèt fòme ki te swiv pa recuit nan yon atmosfè kontwole.
Nòmalize NBK Dènye pwosesis frèt fòme ki te swiv pa recuit pi wo pase pwen transfòmasyon anwo nan yon atmosfè kontwole.

 

 

Tout lòt tib ki aplikab pou chofaj ak tib echanjeur chalè nou ka pwodwi,

 

Estanda Chinwa Steel Klas / No. Estanda Ameriken Steel Klas / No.
GB5310

20G, 15MoG, 12CrMoG,

12Cr2MoG, 15CrMoG,

12Cr1MoVG,

ASTM A106 GR. A,B,C
GB9948 10,20,12CrMo, 15CMo ASTM A53 GR. Yon,B
GB3087 10,20 ASTM A192  
    ASTM A179  
    ASTM A210 A-1,C
    ASTM A333 GR.1% 2cGR3,GR6
    ASTM A334 GR.1% 2cGR3,GR6
    ASTM A209 T1, Ta, Tib
estanda Alman Steel Klas / No. estanda Japonè Steel Klas / No.
DIN17175 ST35.8% 2C ST45.8 JIS G3454 STPG370,STPG410
DIN1629 ST37.0, ST44.{3{3}}, ST52.{5}}} JIS G3461 STB340% 2c STB410, STB440
Britanik estanda Steel Klas / No. estanda Ewopeyen an Steel Klas / No.
BS{0{0}Ⅰ 320 EN10216-1 P195TR1/TR2,P235TR1/TR2,
P265TR1/TR2
BS3059-ⅡS1/S2; TC1/TC2 360,440, EN10216-2
TC1,TC2
195GH% 2cP235GH,
P265GH,

 

 

Aplikasyon:

 

1, Pou evaporator, echanjeur chalè, kondansateur, ekipman transfè chalè ak tiyo menm jan an.

2, lajman itilize nan jaden tretman mekanik, endistri pétrochimique, transpò ak konstriksyon jaden

3, rezon estriktirèl òdinè ak objektif estriktirèl mekanisyen, pou egzanp nan jaden konstriksyon, kote yo pote fulcrum elatriye;

4, transpò likid nan pwojè yo ak gwo ekipman, pou egzanp transpò dlo, lwil oliv, gaz elatriye

5, Èske yo ka itilize nan chodyè presyon ki ba ak mwayen pou transpò likid, pou egzanp tib vapè, gwo tib lafimen, ti tib lafimen, jenere tib elatriye

 

 

Avantaj konpetitif:

 

Asia Leading Steel Pipe & Tube Manufacturer with more than 250,000Tons/Year, >60% anbake nan plis pase 35 Countries.We vize nan manifakti bon jan kalite tiyo & tib ak pri rezonab ak konpetitif, bon kalite pou kliyan mondyal nou yo.

 

 

DIN 2391/EN 10305-4}
Fwad trase oswa frèt woule presizyon tib asye san pwoblèm
Anndan presizyon tib san pwoblèm pou presyon idwolik ak sèvis chanm konpwesyon lè
Aplikasyon: Pou itilize oto; pou itilize machin; Tib silenn lwil oliv; Tib asye redukteur chòk motosiklèt; Silenn enteryè redukteur chòk oto
Gwosè (mm): O.D.:4.0-76 W.T.:0.5-6

 

 

Klas Konpozisyon chimik (%):
C max Si max Mn P max S max
St 35 0.17 0.35 Pi gran pase oswa egal a 0.40 0.025 0.025
St 45 0.21 0.35 Pi gran pase oswa egal a 0.40 0.025 0.025
St 52 0.22 0.55 Mwens pase oswa egal a 1.60 0.025 0.025

 

Steel klas Konpozisyon chimik (%):
Non Steel Nimewo asye C max Si max Mn P max S max Al min
E215 1.0212 0.10 0.05 0.70 0.025 0.025 0.025
E235 1.0308 0.17 0.35 1.20 0.025 0.025 -
E355 1.0580 0.22 0.55 1.60 0.025 0.025 -

 

Pwopriyete mekanik (Mpa):

 


Steel klas
BK zo Mask yo GBK NBK
RMN/mm
min
min RMN/mm
min
min N/mm
min
repete
N/mm
min
min N/mm
min
min N/mm
min
repete
N/mm
min
min
St35 480 6 420 10 420 315 14 315 25 340-470 235 25
St445 580 5 520 8 520 375 12 390 21 440-570 235 21
St52 640 4 580 7 580 420 10 490 22 490-630 355 22

 

Steel klas Valè minimòm pou kondisyon livrezon an
Non Steel Nimewo asye + C + LC + SR + A + N
Rm Mpa A% Rm Mpa A% Rm Mpa ReH Mpa A% Reh Mpa A% Rm Mpa Reh Mpa A%
E215 1.0212 430 8 380 12 380 280 16 280 30 290-430 215 30
E235 1.0308 480 6 420 10 420 350 16 315 25 340-480 235 25
E355 1.0580 640 4 580 7 580 450 10 450 22 490-630 355 22

Tib yo nan estanda sa a yo ekspòte nan Latiki, Almay, Lafrans, UK elatriye Depi 2005

 

Cold Drawn Seamless Steel Pipe Precision Carbon Steel Tube DIN2391 EN10305 ST37 ST52 0Cold Drawn Seamless Steel Pipe Precision Carbon Steel Tube DIN2391 EN10305 ST37 ST52 1

Baj popilè: frèt trase san pwoblèm tiyo asye presizyon kabòn asye tib din2391 en10305 st37 st52, Lachin frèt trase san pwoblèm tiyo asye presizyon kabòn asye tib din2391 en10305 st37 st52 Swèd

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch