Fwad Drawn ASTM A312 TP316L Nerjaveèi asye Tib san pwoblèm SS 316L Inox Tib
Deskripsyon
| Aplikasyon: | Konstriksyon, dekorasyon, endistri, pwodui chimik | Estanda: | DIN, ASTM |
|---|---|---|---|
| Klas asye: | 304 304L 316 316L 310S 321 | Kalite: | San pwoblèm |
| Kalite liy soude: | San pwoblèm | Epesè: | 1-95mm |
| Longè: | 3000mm ~ 6000mm | Fòm: | Wonn.kare.Rektang |
| Dyamèt ekstèn: | 6-762mm | ||
| Limyè segondè: |
TP316L asye pur tib san pwoblèm,ASTM A312 Nerjaveèi Tib san pwoblèm,1.5MM asye pur tib san pwoblèm |
||
Deskripsyon Product
Estanda: ASTM A249, ASTM A268, ASTM A269, ASTM A312, elatriye.
Materyèl: 316, 316L.
Atik: Poli Bright Sifas 316 316L soude tiyo asye pur pou tiyo echapman
Spesifikasyon:
Dyamèt ekstèn: 1.0-1220mm (1/8"-48")
Epesè miray la: 0.1-150mm (SCH 5S- XXS)
Longè: 3m, 5.8m, 6m, 11.8m, oswa kòm demann.
Sifas: marinated, rkwit, poli, klere, eksplozyon sab, liy cheve, elatriye.
ki sa ki 316?
Klas 316 se klas estanda molybdène ki bay, dezyèm nan enpòtans 304 pami asye pur austenitic yo.
Molybdène a bay 316 pi bon pwopriyete ki reziste korozyon an jeneral pase Klas 304, patikilyèman pi wo rezistans nan pitting ak korozyon fant nan anviwònman klori.
Klas 316L, vèsyon an ba kabòn nan 316 epi li se iminitè kont sansibilizasyon (grenn fwontyè presipitasyon carbure).
316/316L konpozisyon chimik
| Materyèl | C | Si | Mn | P | S | Ni | Kr | Mo | N |
| 316 | Mwens pase oswa egal a 0.08 | Mwens oswa egal a 1.00 | Mwens pase oswa egal a 2.00 | Mwens pase oswa egal a 0.045 | Mwens pase oswa egal a 0.03 | 10.0~14.0 | 16.0~18.0 | 2.00~3.00 | - |
| 316L | Mwens pase oswa egal a 0.03 | Mwens oswa egal a 1.00 | Mwens pase oswa egal a 2.00 | Mwens pase oswa egal a 0.045 | Mwens pase oswa egal a 0.03 | 10.0~14.0 | 16.0~18.0 | 2.00~3.00 | Mwens pase oswa egal a 0.10 |
316/316L Pwopriyete mekanik
| Materyèl |
Sede fòs N/mm2 |
Fòs rupture N/mm2 |
Elongasyon (%) |
| 316 | Pi gran pase oswa egal a 205 | Pi gran pase oswa egal a 515 | Pi gran pase oswa egal a 35 |
| 316L | Pi gran pase oswa egal a 170 | Pi gran pase oswa egal a 485 | Pi gran pase oswa egal a 35 |
Konparezon Spesifikasyon Klas
| Klas | UNS No | Old Britanik | Euronorm | Swedish SS | Japonè JIS | ||
| BS | En | Non | Non | ||||
| 316L | S31603 | 316S11 | - | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
316/316L Nerjaveèi aplikasyon pou
Aplikasyon tipik yo enkli:
· Ekipman pou preparasyon manje patikilyèman nan anviwònman klori.
· Bann laboratwa ak ekipman.
· Pano achitekti bò lanmè, balistrad ak taye.
· Ekipman pou bato.
· Resipyan chimik, ki gen ladan pou transpò.
· Echanjeur chalè.
· Trikote oswa soude ekran pou min, karyè ak filtraj dlo.
· Fastener Threaded.
· Springs.
Pwosesis pwodiksyon nan asye pur tiyo soude

Foto pwodwi yo


Baj popilè: frèt trase astm a312 tp316l asye pur tib ss 316l inox tib, Lachin frèt trase astm a312 tp316l asye pur tib san pwoblèm ss 316l inox tib Swèd