ASTM A-333 A333 Gr6 Gr6 Tib / Tib asye san pwoblèm tanperati ki ba
Deskripsyon
| Sètifikasyon: | CE, ISO, BV, SGS | Non pwodwi: | A333 Gr6 Low Tanperati Steel Tiyo |
|---|---|---|---|
| OD: | 12mm{{1}m | Epesè mi: | 0.25mm-45mm |
| Longè: | 1000mm-12000mm | Fòm: | Wonn |
| Estanda: | ASTM, AISI, JIS%, DIN, EN, GB | Teknik: | EWOULE |
| Egzanp: | Pèmèt | Aplikasyon: | Machin |
| Limyè segondè: |
tiyo asye kabòn san pwoblèm,tiyo asye estriktirèl |
||
ASTM A-333 A333 Gr6 Gr6 Tib / Tib asye san pwoblèm tanperati ki ba
| Deskripsyon | A333 Gr6 Low Tanperati Steel Tiyo |
| Tiyo estriktirèl |
A333 Gr6 |
| Tiyo likid | 20# q295b-e, q345b-e |
| Segondè presyon chodyè tib |
20G 15MNG 20MNG 15CrMoG% 2c 12Cr1MoVG St35.8, sa106b, sa106c, sa210a, sa210c, A333P2, A333P11, A33P12, A333P22, A33P36, A333P91, A333P92, A335T2, A335T53T1, A335T53T12 335T23, A335T9 |
| Tiyo |
API SPEC 5L% 2c X42% 2c X52, X60, X65% 2cX70% 2cX80 ASTMA53, ASTM A106, ASTM A333, BS301, BS3602, BS3603, BS3604, PSL1, PSL2, DNV-OS-F101, CSA-Z245 |
| Tiyo alyaj | 4140% 2c 42CrMo, 32CrMo, 15CrMo, |
| Anbalaj | Nwa penti, penti vèni, anbalaj prela |
| Fen | Fen wonn komen, bizote. |
| Pwosesis | Galvanize; koupe; fè fil deyò tiyo a; D'. |
Deskripsyon pwodiksyon an
1) Precision tiyo imaj, Itilizasyon ak Creole



Itilizasyon:Tiyo idwolik, tiyo likid, konstriksyon fizik, aparèy idwolik, pati otomobil, manch asye, kote yo pote, silenn idwolik, silenn konpwesyon ak tiyo idwolik.
Estanda:ISO, JIS, GB, DIN, ASTM, API
2) Desen nan tiyo Precision

3) Tablo spesifikasyon gwosè pwodwi (mm) (zòn ble)

Remak:Nou menm tou nou pwodwi gwosè Customized soti nan lis sa a
4) konpozisyon chimik
Konpozisyon chimik nan tiyo presizyon nan klas itilize souvan
| Estanda | Klas | Konpozisyon chimik (%) | ||||||||||||
| C | sizo | Mn | S | P | Kr | |||||||||
| GB/T699 | 10# | 0.07~0.13 | 0.17~0.37 | 0.35~0.65 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.035 | ||||||||
| GB/T3639-2000 | 20# | 0.17~0.23 | 0.17~0.37 | 0.35~0.65 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.035 | ||||||||
| GB3077-88 | 35# | 0.32~0.39 | 0.17~0.37 | 0.35~0.65 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.035 | ||||||||
| 45# | 0.42~0.50 | 0.17~0.37 | 0.50~0.80 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.035 | |||||||||
| 40kr | 0.37~0.44 | 0.17~0.37 | 0.50~0.80 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.035 | 0.08~1.10 | ||||||||
| 25MN | 0.22~0.29 | 0.17~0.37 | 0.70~1.00 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.25 | ||||||||
| 37Mn5 | 0.30~0.39 | 0.15~0.30 | 1.20~1.50 | Mwens pase oswa egal a 0.015 | Mwens pase oswa egal a 0.020 | |||||||||
5) Pwopriyete mekanik
Pwopriyete mekanik tiyo presizyon komen
| Estanda | Klas | Deziyasyon (%) | ||||||||||||
| Fwad fini (difisil) (BK) | Fwad fini (mou) BKW | |||||||||||||
| UTS (Fòs Tensile Ultim) | pousantaj elongasyon apre ka zo kase | UTS (Fòs Tensile Ultim) | pousantaj elongasyon apre ka zo kase | |||||||||||
| �% 83 b (Mpa) | δ 5(%) | �% 83 b (Mpa) | δ 5(%) | |||||||||||
| GB/T3639-2000 | 10# | Pi gran pase oswa egal a 410 | Pi gran pase oswa egal a 6 | Pi gran pase oswa egal a 375 | Pi gran pase oswa egal a 10 | |||||||||
| GB3077-88 | 20# | Pi gran pase oswa egal a 510 | Pi gran pase oswa egal a 5 | Pi gran pase oswa egal a 450 | Pi gran pase oswa egal a 8 | |||||||||
| 35# | Pi gran pase oswa egal a 590 | Pi gran pase oswa egal a 4 | Pi gran pase oswa egal a 550 | Pi gran pase oswa egal a 6 | ||||||||||
| 45# | Pi gran pase oswa egal a 645 | Pi gran pase oswa egal a 4 | Pi gran pase oswa egal a 630 | Pi gran pase oswa egal a 5 | ||||||||||
| 40kr | Pi gran pase oswa egal a 784 | Pi gran pase oswa egal a 12 | ||||||||||||
| 37Mn5 | Pi gran pase oswa egal a 784 | Pi gran pase oswa egal a 12 | ||||||||||||
Remak:
Fini frèt (difisil):Tib pa sibi tretman chalè apre fòm final la frèt epi, kidonk, gen yon rezistans olye segondè nan deformation.
Fini frèt (mou):Se tretman chalè final la ki te swiv pa desen frèt ki enplike deformation limite. Apwopriye plis pwosesis pèmèt yon sèten degre nan fòme frèt (egzanp koube, agrandi)
6) endistri aplikasyon pwodwi

Jaden aplikasyon:
Pwosesis mekanik, fabrikasyon machin, otomobil
7) Kontwòl Kalite
A. Ekipman Pwodiksyon Avanse

B. Koule Pwodiksyon
C. Travayè ki gen konpetans ak ki kalifye, fòmasyon ak tès anvan travay

D. Fè egzateman sistèm kontwòl kalite

8) Anbalaj & Shipping
A) Metòd anbalaj
Ti gwosè nan pakèt, gwo gwosè nan esansyèl, ak bouchon plastik pou pwoteje tou de bout, anbalaj navigab oswa selon demann kliyan an.

B) Fason Shipping
Dapre demann kliyan an.
Anjeneral pa lanmè, pa lè, pa tren oswa rivyè-ak-lanmè transpò kowòdone.
FAQ
K: Ki sa ki sou tèm peman ou a?
A: Anjeneral T/T oswa L/C, 30% depo ak 70% anvan livrezon.
K: e dat livrezon estanda ou a?
A: 30 jou apre li fin resevwa depo
K: Kouman sou kapasite ou a?
A: Pou tiyo asye, 50,000 tòn pa mwa, 600,000 tòn pa ane. Pou ekipman tiyo, 30,000 tòn pa ane
K: e pakè ou a?
A: Anjeneral dapre demann kliyan an.
Enfòmasyon komen anbalaj: Ti gwosè nan pake, gwo gwosè nan esansyèl, kèk gwosè ak bouchon plastik pwoteje tou de bout, anbalaj navigab.
K: Ki sa ki mache prensipal ou a ak kliyan prensipal yo?
A: Nou gen 12 ane eksperyans sou tiyo asye ak ekipman tiyo. Mache prensipal nou an gen ladan Lachin, Singapore elatriye Kliyan prensipal ki gen ladan HYST, Keppel gwoup elatriye.
K: Si pwodwi yo gen kèk pwoblèm kalite, ki jan ou ta fè fas ak?
A: Nou pral responsab pou tout pwoblèm kalite nou yo.
K: Ki jan yo ka resevwa pri egzat / sitasyon nan men ou?
A: Tanpri tanpri di nou detay anba a epi nou pral voye sitasyon nou an ba ou ASAP:
1) Dyamèt ekstèn tiyo a
2) epesè miray la
3) Fòm Seksyon (wonn, kare elatriye)
4) Longè pou chak tiyo
5) klas asye
6) Creole (egzanp: API 5L)
7) Kantite lòd
8) Deziyasyon (BK, BKW elatriye)
9) Kondisyon komès
PS: plis enfòmasyon detaye ou klarifye, plis pri egzak nou te bay.
Baj popilè: astm a-333 a333 gr6 gr6 ki ba tanperati san pwoblèm tiyo asye / tib, Lachin astm a-333 a333 gr6 gr6 tanperati ki ba san pwoblèm tiyo asye / tib founisè
Ou ka renmen tou
Voye rechèch