The 436 stainless steel coil is a high-quality product with excellent performance in various industrial applications. With a thickness range of 0.3mm to 3mm and a width of 1000mm to 1500mm, this coil can be tailored to meet the requirements of any customer.
Voye rechèch
Chat kounye a

Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.

Pwodwi Entwodiksyon

 

Stainless Steel 436 Coil

The 436 stainless steel coil is a high-quality product with excellent performance in various industrial applications. With a thickness range of 0.3mm to 3mm and a width of 1000mm to 1500mm, this coil can be tailored to meet the requirements of any customer.




Model: 436
UNS number: S43600
●Chemical composition of 436 steel①:
Carbon C: Less than or equal to 0.12
Manganese Mn: Less than or equal to 1.00
Silicon Si: Less than or equal to 1.00
Chromium Cr: 16.0~18.0
Nickel Ni②:-
Phosphorus P: Less than or equal to 0.04
Sulfur S: Less than or equal to 0.03
Molybdenum Mo: 0.75~1.25
Niobium Nb: (5C~0.80)