Èske C276 se yon alyaj nikèl?
Gnee Steel stocks Hastelloy C-276 nickel alloy plate in thicknesses ranging from 3/16 inch (4.8 mm) to 2 ½ inches (63.5 mm) and is one of the most versatile corrosion-resistant materials available for applications such as chemical and petrochemical processing, flue gas desulfurization, pulp and paper equipment, industrial waste and air pollution control.
Hastelloy C -276 ki disponib nan:
| 3/16" | 1/4" | 3/8" | 1/2" | 5/8" | 3/4" |
| 4.8mm | 6.3mm | 9.5mm | 12.7mm | 15.9mm | 19mm |
| 1" | 1 1/4" | 1 1/2" | 1 3/4" | 2" | 2 1/2" |
| 25.4mm | 31.8mm | 38.1mm | 44.5mm | 50.8mm | 63.5mm |


Hastelloy C -276 Nikèl Plak Alloy (UNS N10276) se yon alyaj nikèl-molibdèn-chromium-fè-tungsten ki se youn nan alyaj ki pi korozyon rezistan ki disponib. Kontni an segondè molibden bay li rezistans nan korozyon lokalize tankou opozisyon. Kabòn ki ba a minimize presipitasyon nan karsid pandan soude, kidonk kenbe rezistans nan kowozyon intergranular nan zòn nan chalè ki afekte nan jwenti a soude.
Hastelloy C -276 Nikèl plak alyaj tou gen bon fòs tanperati ki wo ak modere rezistans oksidasyon, byenke alyaj la pral evantyèlman fòme frajil segondè presipite tanperati.
Hastelloy C -276 (UNS N10276) Fèy Spesifikasyon Apèsi sou lekòl la
Yon alyaj nikèl-molibden-chromium ak ekselan rezistans korozyon nan tou de oksidant ak diminye anviwònman
Pwopriyete jeneral
Aplikasyon
Estanda
Analiz chimik
Pwopriyete fizik
Pwopriyete mekanik
Rezistans korozyon
Done Faktori