Ki diferans ki genyen ant Hastelloy C22 ak C276?
1. Materyèl diferan
1. Hastelloy C22: 56NI-13MO-22CR-3FE-3W-2.5CO-0.5MN-0. 35V-0.08SI-0.01C.
2. Hastelloy C276: 57NI-16MO-16CR-5FE-4W-2.5CO-1MN-0.35V -0.08SI-0.01C. C-276 Hastelloy se yon alyaj nikèl-molybdène-kwòm-fè-tungstèn ki baze sou nikèl e li pi reziste korozyon nan mitan materyèl metal modèn. Sitou rezistan a klò mouye, divès kalite klori oksidan, solisyon sèl klori, asid silfirik ak sèl oksidan, e li gen bon rezistans korozyon nan asid idroklorik tanperati ki ba ak mwayen.


2. Diferan materyèl soude
1. Hastelloy C22: C22 materyèl soude yo soude fil ERnicrmo -10 ak baton soude Enicrmo -10.
2. Hastelloy C276: C276 soude consommables yo soude fil ERnicrmo -4 ak soude baton Enicrmo -4.
3. Diferan dansite
1. Hastelloy C22: Dansite C22 alyaj se 8.7.
2. Hastelloy C276: Dansite C276 alyaj se 8.9.