What are the differences between Inconel 600 flanges and Inconel 718 alloy flanges?
01

Ki diferans ki genyen ant bride Inconel 600 ak bride alyaj Inconel 718?

Brides Inconel 600 yo itilize prensipalman pou rezistans oksidasyon segondè -tanperati a epi yo renome pou rezistans ekselan yo nan klori-fè estrès korozyon krak, ki fè yo apwopriye pou aplikasyon pou tretman chalè-. Kontrèman, Inconel 718 bride se yon alyaj presipitasyon -di ak fòs siyifikativman pi wo, lajman ki itilize nan ayewospasyal, motè jè, ak lòt gwo -fòs, segondè- anviwònman tanperati. Diferans prensipal la chita nan konpozisyon yo ak pwopriyete mekanik ki kapab lakòz yo: Brides Inconel 600 yo se bride alyaj nikèl ki wo - ak ekselan rezistans korozyon; pandan y ap Inconel 718 brides yo pi wo -fòs, laj-brides alyaj redi ki apwopriye pou aplikasyon estriktirèl.

02

Èske Inconel 600 alyaj ka soude?

Inconel 600 alyaj ka soude lè l sèvi avèk divès metòd, tankou tengstèn gaz inaktif soude (GTAW) oswa soude agon arc (TIG). Lòt metòd enkli gaz metal arc soude (GMAW), gaz metal arc soude (MIG), ak plasma arc soude (PAW).

Inconel 600 Alloy

 

Brides Inconel 600 yo favorize nan endistri asye ak soude akòz nati ki pa-mayetik yo ak ekselan soudabilite. Yo souvan itilize nan fabrike nan djenn tèrmokòl ak tib piroliz EDC. Akòz gwo -rezistans presyon yo, yo itilize bride Inconel 600 tou nan réacteurs dlo presyon pou kontwole plak dèlko vapè. Anplis de sa, yo itilize nan réacteurs nikleyè pou kontwole divès kalite resipyan ak kanalizasyon. Lòt aplikasyon pou Inconel 600 bride yo enkli foyer roulo, kettles distilasyon, ak founo moufle.

 

Inconel 718 bride yo lajman ki itilize nan perçage lwil oliv, pétrochimique, jenerasyon pouvwa, pwosesis gaz natirèl, fabrikasyon ekipman chimik, fabrikasyon ekipman pharmaceutique, echanjeur chalè, ak kondansateur. Klèman, prèske chak endistri depann sou bride sa yo. Brides Inconel yo se yon eleman endispansab nan endistri manifakti ak pwosesis.

 

Spesifikasyon Inconel 600/601/625/718 bride

Spesifikasyon Inconel bride:ASTM B564 / ASME SB564
Dimansyon estanda:ANSI/ASME B16.5, B 16.47 Seri A & B, B16.48, BS4504, BS 10, EN-1092, DIN, elatriye.
Estanda:ANSI brides, ASME brides, BS brides, DIN brides, EN brides, elatriye.
Gwosè:1/2" (15 NB) pou 48" (1200NB)
Klas / Presyon:150 #, 300 #, 600 #, 900 #, 1500 #, 2500 #, PN6, PN10, PN16, PN25, PN40, PN64 elatriye.
Kalite figi bride:Flate Face (FF), Raised Face (RF), Joint Kalite Ring (RTJ)
Bride DIN:DIN 2527, 2566, 2573, 2576, 2641,2642, 2655, 2656, 2627, 2628, 2629, 2631, 2632, 2633, 2634, 2636, 2636, 2636, 2636, 2637 2673.
Bride JIS:JIS B2220 5K, JIS B2220 10K, JIS B2220 16K, JIS B2220 20K
BS bride:BS4504 PN 6, BS 4504 PN 10, BS4504 PN 16, BS4504 PN 25, BS4504 PN 40, BS 4504 PN 64, BS 4504 PN 100, BS 4504 PN 1604, BS 4504 PN 165 10, BS Table D, BS Table E, BS Table F, BS Table H.

 

Inconel 600/718 Bride Klas ekivalan

STANDARD UNS WERKSTOFF NR. AFNOR GOST OSWA BS JIS EN
Inconel 600 N06600 2.4816 NC15FE11M МНЖМц 28-2,5-1,5 ЭИ868 NA 13 NCF 600 NiCr15Fe
Inconel 718 N07718 2.4668 - - - - NCF 718 -

 

Konpozisyon chimik nan Inconel 600/718 bride

Klas Ni Fe C Mn Si Cu Kr S Mo Co Al Ti Nb
600 72.0 min 6.0 - 10.0 0.15 max 1.0 max 0.5 max 0.5 max 14.0 - 17.0 0.015 max - - - - -
601 58.0 – 63.0 Balans 0.10 max 1.0 max 0.50 max 1.0 max 21.0 – 25.0 0.015 max 8.0-10.0 - 1.0 – 1.7 - -
625 58.0 max 5.0 max .10 max .50 max .50 max - 20.0 - 23.0 .015 max 8.0 - 10.0 1.0 max .40 max .40 max 3.15 - 4.15
718 50 - 55 - 0.08 max 0.35 max 0.35 max 0.3 max 17 - 21 .015 max 2.8 - 3.3 1.0 max - - -

 

Pwopriyete mekanik nan Inconel 600/718 bride

Klas Tensile (psi) .2% Sede (psi) elongasyon (%)
600 95,000 45,000 40
601 80,000 30,000 35

 

Konparezon pwopriyete mekanik: Inconel 600 Flange vs Inconel 718 Flange

Pwopriyete Inconel 600 bride (rekuit) Inconel 718 Flange (ki gen laj / trete solisyon + ki gen laj)
Fòs rupture (tanperati chanm) 550 - 690 MPa 1240 - 1380 MPa
Fòs Sede (0.2% Offset, Tanperati chanm) 240 - 350 MPa 1030 - 1170 MPa
Elongasyon 30 – 45 % 12 – 20 %
Rediksyon nan zòn 45 – 55 % 15 – 25 %
Dite (tanperati chanm) 65 - 90 HRB 35 - 45 HRC
Modil Elastisite 207 GPa 205 GPa
Fòs fatig (wotasyon gwo bout bwa, tanperati chanm) 270 - 310 MPa 450 - 550 MPa
Chea fòs ≈ 520 MPa ≈ 830 MPa
Severite enpak (Charpy V-Notch, Tanperati chanm) > 100 J 30 – 60 J
Segondè -Fòs Tensile Tanperati (650 degre) ≈ 300 MPa ≈ 1000 MPa
Gwo -Fòs Sede Tanperati (650 degre) ≈ 150 MPa ≈ 850 MPa
Fòs rupture ranpe (700 degre, 1000h) ≈ 60 MPa ≈ 250 MPa
Maksimòm Tanperati Sèvis Rekòmande (Kontinyèl) ≈ 1095 degre ≈ 700 degre
Tanperati Minimòm Sèvis ≈ -250 degre ≈ -250 degre
Koyefisyan ekspansyon tèmik (20-100 degre) 13.3 μm/m· degre 13.0 μm/m· degre
Kondiktivite tèmik (100 degre) 14.8 W/m·K 11.4 W/m·K
Kapasite chalè espesifik (20 degre) 460 J/kg·K 435 J/kg·K
Dansite 8.47 g / cm³ 8.19 g / cm³
Pwopòsyon Poisson a 0.29 0.29

 

Poukisa chwazi Gnee kòm founisè alyaj ki baze sou nikèl ou.{0}}

✅ Plis pase 18 ane eksperyans nan ekspòtasyon, pwodwi vann nan plis pase 80 peyi

✅ Sètifye pa ISO, SGS, ak BV

✅ Envantè mondyal Inconel, Hastelloy, Incoloy, ak Monel alyaj tib, plak, ak ba

✅ Sèvis pwosesis koutim ki disponib - ki gen ladan koupe, polisaj, machin CNC, ak anbalaj

✅ Livrezon rapid nan 7-15 jou, sipòte pa patnè lojistik mondyal yo

📦 Anbalaj ak livrezon

Tout pwodwi asye pur yo pake lè l sèvi avèk metòd sa yo:

Palèt an bwa oswa kès

Anbalaj prèv imidite-

Etikèt ak nimewo founo, estanda, ak etikèt gwosè

Anbake atravè lemond pa lanmè, lè, oswa eksprime

 