Tablo pwa bar wonn Inconel 601, 601 alyaj pwa bar wonn tablo, 601 kalkilatris pwa bar wonn (kilogram), Inconel 601 pwa bar wonn pou chak mèt, Inconel 601 alyaj pwa wonn tablo pwa, nikèl 601 tablo pwa wonn bar PDF, 601 alyaj fòmil kalkil pwa bar kare UNS6, fòmil kalkil UNS6 pwa bar kare 6. kalkilatris pwa ba, 601 kalkilatris pwa ba wonn, kalkilatris pwa bar wonn, 601 tablo pwa bar, nikèl 601 tablo pwa bar, Alloy 601 tablo pwa ba wonn.
Inconel 601 (UNS NO6601) ba wonn se yon alyaj kwòm segondè -nikèl- ak yon dansite apeprè 8.11 g/cm³ (0.293 lb/in³). Yon bar wonn tipik 1-pous dyamèt peze apeprè 2.67 liv pou chak pye (3.97 kg / m), pandan y ap yon ba wonn dyamèt 2-pous peze apeprè 10.68 liv pou chak pye (15.9 kg / m).
Tablo pwa bar wonn
| Dia | Pwa | Dia | Pwa |
|---|---|---|---|
| (mm) | pou chak mèt (kg) | (nan) | pou chak mèt (kg) |
| 3mm | 0.06 | 1/8″ | 0.06 |
| 4mm | 0.10 | 3/16″ | 0.14 |
| 5mm | 0.16 | 1/4″ | 0.25 |
| 6mm | 0.22 | 5/16″ | 0.39 |
| 7mm | 0.30 | 3/8″ | 0.56 |
| 8mm | 0.40 | 7/16″ | 0.77 |
| 10mm | 0.62 | 1/2″ | 1.00 |
| 12mm | 0.89 | 9/16″ | 1.22 |
| 14mm | 1.22 | 5/8″ | 1.56 |
| 15mm | 1.40 | 11/16″ | 1.89 |
| 16mm | 1.59 | 3/4″ | 2.25 |
| 18mm | 2.01 | 7/8″ | 3.07 |
| 20mm | 2.48 | 1″ | 4.03 |
| 22mm | 3.00 | ||
| 24mm | 3.57 | ||
| 25mm | 3.88 |
Tablo pwa bar wonn an mm, Kg, ft
| Gwosè an mm | Pwa Mwayèn | |
|---|---|---|
| KG/MTR | KG/FT | |
| 10 | 0.62 | 0.18 |
| 12 | 0.90 | 0.30 |
| 14 | 1.20 | 0.40 |
| 16 | 1.60 | 0.50 |
| 18 | 2.00 | 0.60 |
| 20 | 2.50 | 0.80 |
| 22 | 3.00 | 0.90 |
| 24 | 3.56 | 1.08 |
| 25 | 3.90 | 1.20 |
| 28 | 4.80 | 1.50 |
| 30 | 5.55 | 1.69 |
| 32 | 6.30 | 1.90 |
| 34 | 7.14 | 2.18 |
| 36 | 8.00 | 2.44 |
| 40 | 9.90 | 3.00 |
| 45 | 12.49 | 3.81 |
| 50 | 15.40 | 4.70 |
| 56 | 19.34 | 5.89 |
| 60 | 22.20 | 6.80 |
| 63 | 24.47 | 7.46 |
| 63.5 | 24.86 | 7.58 |
| 65 | 26.05 | 7.94 |
| 70 | 30.20 | 9.20 |
| 73 | 32.86 | 10.00 |
| 75 | 34.72 | 10.58 |
| 78 | 37.51 | 11.43 |
| 80 | 39.50 | 12.00 |
| 83 | 42.47 | 12.95 |
| 85 | 44.55 | 13.58 |
| 90 | 50.00 | 15.20 |
| 92 | 52.19 | 15.91 |
| 93 | 53.39 | 16.27 |
| 95 | 55.65 | 16.95 |
| 100 | 61.66 | 18.79 |
| 105 | 67.98 | 20.72 |
| 110 | 74.60 | 22.74 |
| 115 | 81.64 | 24.88 |
| 125 | 96.34 | 29.36 |