Inconel 600 tablo pwa ba wonn, Nikèl 600 pwa ba wonn pou chak mèt, Inconel 600 Alloy tablo pwa wonn ba, 600 alyaj pwa tablo pwa.
Inconel 600 Round Bar Tolerans Tablo
| Dia | Pwa | Dia | Pwa |
|---|---|---|---|
| (mm) | pou chak mèt (kg) | (nan) | pou chak mèt (kg) |
| 3mm | 0.06 | 1/8″ | 0.06 |
| 4mm | 0.10 | 3/16″ | 0.14 |
| 5mm | 0.16 | 1/4″ | 0.25 |
| 6mm | 0.22 | 5/16″ | 0.39 |
| 7mm | 0.30 | 3/8″ | 0.56 |
| 8mm | 0.40 | 7/16″ | 0.77 |
| 10mm | 0.62 | 1/2″ | 1.00 |
| 12mm | 0.89 | 9/16″ | 1.22 |
| 14mm | 1.22 | 5/8″ | 1.56 |
| 15mm | 1.40 | 11/16″ | 1.89 |
| 16mm | 1.59 | 3/4″ | 2.25 |
| 18mm | 2.01 | 7/8″ | 3.07 |
| 20mm | 2.48 | 1″ | 4.03 |
| 22mm | 3.00 | ||
| 24mm | 3.57 | ||
| 25mm | 3.88 |
Founisè stock Inconel 600 bar. Nikèl 600 metrik tablo pwa ba wonn, 12mm tablo pwa bar wonn.