ASTM B165 UNS N04400 alyaj san pwoblèm tiyo pou endistri pétrochimique

 
ASTM B165 UNS N04400 Alloy san pwoblèm tiyo pou endistri pétrochimique
ASTM B165 UNS NO4400 Alloy seamless pipe for petrochemical industry
01

ASTM B165 UNS N04400 Alloy san pwoblèm tiyo pou endistri pétrochimique

Tiyo san pwoblèm ASTM B165 UNS NO4400, ke yo rele tou Monel 400 tiyo san pwoblèm, enpòtan anpil nan endistri pétrochimique akòz rezistans ekselan li nan dlo lanmè, asid ak korozyon alkali, ak bon pwopriyete mekanik sou yon pakèt tanperati. Konsiderasyon kle yo enkli kapasite li pou kenbe tèt ak anviwònman ki trè korozivite tankou sa yo jwenn nan plant chimik, fòs mekanik li yo, ak konvnab li pou aplikasyon pou tanperati ki wo jiska 538 degre (1000 degre F). Li disponib nan kondisyon frèt-travay, rkwit, oswa estrès-soulajman nan yon varyete gwosè ak epesè.

02

ki sa ki UNS N04400?

UNS N04400 refere a Monel 400, yon alyaj nikèl -kwiv li te ye pou gwo fòs li yo ak ekselan rezistans korozyon, ki fè li apwopriye pou itilize nan yon varyete anviwònman korozivite, ki gen ladan dlo lanmè, asid, ak alkali. Materyèl sa a lajman itilize nan jeni lanmè, pwosesis chimik, ak endistri lwil oliv ak gaz.

UNS N04400
 
 

ASTM B165 UNS N04400 Tiyo Spesifikasyon

Spesifikasyon ASTM ASTM B 165 ASME SB 165 / ASTM B 725 ASME SB 725, UNS 4400 Tiyo
Estanda ASTM, ASME, JIS, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB
ASTM B165 monel 400 san pwoblèm gwosè tiyo 4 a 219mm WT: 0.5 a 20mm
UNS N04400 Gwosè tiyo soude 5.0 - 1219.2 mm
Monel WERKSTOFF NR. 2.4360 EFW Gwosè tiyo 5.0 - 1219.2 mm
Swg & Bwg 12 Swg., 10 Swg., 16 Swg., 14 Swg., 20 Swg., 18 Swg.,
400 Monel Pipe Orè XS, SCH30, SCH40, XXS, SCH80, SCH120, SCH60, SCH140, STD, SCH10, SCH10S, SCH40S, SCH80, SCH20, SCH5, SCH160
monel 400 tiyo Longè Double Random, Single Random, Standard & Koupe longè tiyo
Fini Poli, AP (Annealed & marinated), BA (Klere & Recuit), MF, NO.1, NO.4, 2B, BA, HL, 8K, Miwa fini, elatriye
Fòm monel 400 yo disponib nan fòm wonn, kare, kre, rektangilè, idwolik, mawonnen, tiyo dwat, "U" fòm, pan gato bobin elatriye.
Kalite 400 tiyo alyaj San pwoblèm / ERW / EFW / soude / fabrike / CDW / DOM / CEW monel 400
monel 400 tiyo Fen Plain Fen, Bizote Fen, Treaded Tiyo, Vise pwent
Make sou Alloy 400 Tiyo Tout tiyo ASTM B165 monel 400 yo make jan sa a: estanda, klas, OD, epesè, longè, nimewo chalè (oswa selon demann kliyan an.)
Aplikasyon nan tiyo monel 400 Tiyo letye, tiyo lwil oliv, tiyo gaz, tiyo likid, tiyo chodyè pou endistri chimik

 

Monel 400 tiyo san pwoblèm Pwopriyete mekanik

Materyèl Kondisyon OD
pous (mm)
Fòs rupture
min ksi (MPa)
Fòs Sede (0.2% Offset)
min psi (MPa)
Elongasyon nan 2 pous oswa 50 mm (oswa 4 D) min%
alyaj
UNS N04400
Rkwit Mwens pase oswa egal a 5 pous (127 mm) 70(480) 28(195) 35
>5 pous (127 mm) 70(480) 25(170) 35
Estrès-soulaje Tout gwosè 85(585) 55(380) 15

 

Tablo orè nan ASTM B165 monel 400 tiyo san pwoblèm

1/8 "IPS (.405" OD)

3 1/2" IPS (4.000" OD)

SCH 40, 80

SCH 10, 40, 80, 160, XXH

1/4 "IPS (.540" OD)

4" IPS (4.500" OD)

SCH 10, 40, 80

SCH 10, 40, 80, 160, XXH

3/8 "IPS (.675" OD)

5" IPS (5.563" OD)

SCH 10, 40, 80

SCH 10, 40, 80, 160, XXH

1/2 "IPS (.840" OD)

6" IPS (6.625" OD)

SCH 5, 10, 40, 80, 160, XXH

SCH 5, 10, 40, 80, 120, 160, XXH

3/4 "IPS (1.050" OD)

8 "IPS (8.625" OD)

SCH 10, 40, 80, 160, XXH

SCH 5, 10, 40, 80, 120, 160, XXH

1" IPS:(1.315′OD)

10" IPS (10.750" OD)

SCH 5, 10, 40, 80, 160, XXH

SCH 10, 20, 40, 80 (.500), VRE 80 (.500)

1-1/4 "IPS (1.660" OD)

12" IPS (12.750" OD)

SCH 10, 40, 80, 160, XXH

SCH 10, 20, 40(.375), TRUE40(.406), SCH80(.500)

1-1/2 "IPS (1.900" OD)

14" IPS (14.000" OD)

SCH 10, 40, 80, 160, XXH

SCH10 (.188), SCH40 (.375)

2" IPS (2.375" OD)

16" IPS (16.000" OD)

SCH 10, 40, 80, 160, XXH

SCH10(.188), SCH40(.375)

2 1/2" IPS(2.875"OD)

18" IPS (18.000" OD)

SCH 10, 40, 80, 160, XXH

SCH-40 (.375)

3" IPS (3.500" OD)

 

SCH 5, 10, 40, 80, 160, XXH

 

 

Monel 400 tiyo Tablo konpozisyon chimik

Klas C Mn Si S Cu Fe Ni Kr
Monel 400 0.30 max 2.00 max 0.50 max 0.24 max 28.0-34.0 2.50 max 63.00 min –
 

ASME SB 165 san pwoblèm Monel 400 tiyo Mechanical Behavior

Eleman Dansite Pwen k ap fonn Fòs rupture Fòs Sede (0.2% Offset) Elongasyon
Monel 400 8.8 g/cm3 1350 degre (2460 degre F) Psi - 80,000, MPa - 550 Psi - 35,000, MPa - 240 40 %

 

Aplikasyon komen nan endistri pétrochimique
Anviwònman korozivite: Yo itilize nan aplikasyon ki ekspoze a medya korozif tankou asid ak sèl.
Pwosesis chimik: Apwopriye pou fabrike ekipman tankou réacteurs chimik, echanjeur chalè, tank depo, kanalizasyon, ak ponp.
Pwosesis lwil brit: Yo itilize pou kouvri kolòn distilasyon lwil brit.
Kontwòl Polisyon ak Tretman Dechè: Yo itilize nan tretman dechè endistriyèl ak sistèm kontwòl polisyon.
Pwodiksyon idrokarbone klò: Yo itilize nan ponp ak tiyo pou pwodiksyon idrokarbur klò.

Gnee Steel

 

Konsènan Gnee Steel

Gnee Steel espesyalize nan pwodiksyon ak vann divès kalite alyaj ki baze sou nikèl -, ki gen ladan nikèl 201, nikèl 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 625, Inconel, Inconel71 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, ak alyaj wo-tanperati. Pwodwi Gnee Steel yo lajman itilize nan ayewospasyal, chimik, pouvwa elektrik, otomobil, ak aplikasyon pou enèji nikleyè. Nou ofri tou solisyon alyaj Customized adapte a bezwen kliyan yo. Pou demann pri alyaj oswa solisyon alyaj Customized, tanpri kontakte nou pou yon quote nanss@gneesteel.com.