Ekipman Hastelloy C22 yo te fè soti nan yon alyaj nikèl-chromium-molibdèn li te ye pou rezistans siperyè korozyon yo nan yon varyete de anviwònman piman bouk, ki gen ladan sa yo ki gen asid oksidant, diminye asid, klorid, ak lòt pwodwi chimik korozivite. Yo souvan itilize nan pwosesis chimik, kontwòl polisyon, ak lòt endistri kote rezistans korozyon ak pèfòmans segondè-tanperati yo kritik.

Hastelloy C22 Fittings - A Complete Guide

Steel Gnee

 

Ki pwopriyete mekanik Hastelloy C22?

Materyèl Hastelloy C22 gen pwopriyete ekselan mekanik. Fòs rupture li se omwen 100 ksi ak fòs sede li yo se omwen 45 ksi. Anplis de sa, li fasil machin ak soude.

Hastelloy C22

Hastelloy C22 ekipman fabrikasyon pwosesis

Hastelloy C22 Fittings Manufacturing Process

Konpòtman mekanik nan Nikèl C22 ekipman tiyo

Eleman Dansite Pwen k ap fonn Fòs rupture Sede fòs (0.2%konpanse) Elongasyon
Hastelloy C22 8.69 g/cm3 1399 degre (2550 degre F) PSI - 1,00,000, MPa - 690 PSI - 45000, MPA - 310 45 %

Tablo konpozisyon nan ASTM B366 UNS N06022 ekipman

Egalize C Mn Si S CO NI Cr Fe Mwa P
C22 0.010 max 0.50 max 0.08 Max 0.02 Max 2.50 max 50.015 min* 20.00 – 22.50 2.00 – 6.00 12.50 – 14.50 0.02 Max

Hastelloy C22 tiyo ekipman pou dimansyon

Gwosè tiyo nominal Tout ekipman Tout ekipman Tout ekipman Koud/ tees 180 degre retounen viraj 180 degre retounen viraj 180 DEG retounen viraj Rediktè Kapsin
NP OD nan Bevel (1), (2) Id nan fen
(1), (3), (4)
Epesè miray (3) Sant-a-fen dimansyon a, b, c, m Sant-a-sant o Do-a-fas k Aliyman nan fini u Longè an jeneral H Longè an jeneral e
½ a 2½ 0.06
-0.03
0.03 Pa mwens pase 87.5% nan epesè nominal 0.06 0.25 0.25 0.03 0.06 0.12
3 a 3 ½ 0.06 0.06 Pa mwens pase 87.5% nan epesè nominal 0.06 0.25 0.25 0.03 0.06 0.12
4 0.06 0.06 Pa mwens pase 87.5% nan epesè nominal 0.06 0.25 0.25 0.03 0.06 0.12
5 a 8 0.09
-0.06
0.06 Pa mwens pase 87.5% nan epesè nominal 0.06 0.25 0.25 0.03 0.06 0.25
10 a 18 0.16
-0.12
0.12 Pa mwens pase 87.5% nan epesè nominal 0.09 0.38 0.25 0.06 0.09 0.25
20 a 24 0.25
-0.19
0.19 Pa mwens pase 87.5% nan epesè nominal 0.09 0.38 0.25 0.06 0.09 0.25
26 a 30 0.25
-0.19
0.19 Pa mwens pase 87.5% nan epesè nominal 0.12 … … … 0.19 0.38
32 a 48 0.25
-0.19
0.19 Pa mwens pase 87.5% nan epesè nominal 0.19 … … … 0.19 0.38
Gnee Steel

 

Sou asye goudwon

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, ak gwo tanperati alyaj. Pwodwi Gnee Steel la yo lajman itilize nan avyon, chimik, pouvwa elektrik, otomobil, ak aplikasyon pou enèji nikleyè. Nou ofri tou solisyon alyaj Customized pwepare a bezwen kliyan. Pou kesyon prix alyaj oswa solisyon alyaj Customized, tanpri kontakte nou pou yon quote nanss@gneesteel.com.