Inconel 718 Tib rektangilè
Gnee Group ofri nikèl alyaj Inconel 718 nan yon varyete de fòm, ki gen ladan:
Bars
Fil
Dra
Minè
Tib
Balans
Tib san pwoblèm ak soude
Baton soude
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Gnee alyaj 718 rektangilè pipinjg prezante
Nikèl Alloy 718 tiyo, ASTM B983 Inconel 718 Tib, Inconel 718 tiyo san pwoblèm, Inconel 718 Tib san pwoblèm, Inconel 718 Tib, Inconel Alloy 718 tiyo, Nikèl alyaj 718 Pipe/Tube Distribitè, Alloy 2.468 Pipe, unss N077, Pye N07, N07 PIPE, PIPE, PIPE, PIPE, PIPE, PIPE, PIPE, NIKEL N07, PIPE, PIPE, NIKEL N07 PIPE, NIKEL N07 PIPE, NICKEL N07 PIPE, Lachin ASTM B983 ALLOY 718 Founisè tiyo san pwoblèm.
Yo itilize tiyo Inconel 718 nan pwodiksyon asid nitrik, nan ekipman an kòm yon sipò kadriyaj katalis, epi tou nan konpozan brûler. Li gen ekselan rezistans korozyon ak pi wo fòs, ak estabilite nan konpozisyon chimik li yo ede travay nan yon seri tanperati lajè. Li se vo konsidere konbinezon an nan CHROMIUM, Cobalt, chrome, nikèl, elatriye Li se lajman ki itilize nan jaden divès kalite nan endistri. Inconel 718 se tiyo san pwoblèm souvan itilize fè tiyo pou wokèt gaz likid, endistri avyon, dezabiye dlo tounen, aparèy chofaj, tank izolasyon, kondansateur, refòmatè amonyak, elatriye Li tou sèvi endistri chimik la, endistri petrochimik, endistri siman, refineries, kaka ak papye, ak anpil lòt endistri yo.
| Estanda | Inconel 718 |
| Ògje | N07718 |
| WERKSTOFF NR. | 2.4668 |
GNEE 718 tiyo kare ak tib spesifikasyon
Spesifikasyon:ASTM B444, ASTM B751, ASTM B829, ASTM B775, ASTM B705, ASTM B704, AMS 5581, ISO 6207, BS 3074NA21, DIN 17751,
Creole:ASTM, ASME ak API
Gwosè tiyo:15 NB jiska 718 NB nan Sch 5s, 10s, 10, 20, 40s, 40, STD, 60, 80s, 80, xs, 100, 120, 140, 160 & xxs
Gwosè tib:1 mm OD jiska 254 mm OD nan 0. 2 a 20 mm epesè.
Kalite:San pwoblèm / erw / soude / fabrike
Longè:Single o aza, doub o aza & obligatwa longè, koupe longè
Fen:Fen plenn, fen bizote, treaded
Gnee Ready Stock nan Inconel 718 Alloy Tubing
| Inconel alyaj 718 tib | Alyaj 718 tib deyò dyamèt |
| Inconel 718 Custom Tib | Inconel 718 segondè presyon tib |
| 718 tib inconel | Inconel 718 frèt trase tib |
| 718 Inconel mens miray tib | 718 estanda tib inconel |
| Alyaj 718 wonn tib | Asme sb 983 718 inconel alyaj tib |
| Inconel 718 tib echanjeur chalè | Alloy 718 Tib grosist |
| 718 Inconel Endistriyèl Tib | Inconel alyaj 718 tib kapilè |
| Inconel alyaj 718 mens miray soude tib | Nikèl alyaj 718 tib |
| ASTM B 983 718 Inconel Tubing | 718 Inconel alyaj erw tib |
Gnee alyaj 718 orè tib kare
| Aparèy mesi | Ranje epesè (pous) | Valè tipik (pous) |
|---|---|---|
| 22 | 0.025 – 0.029 | 0.028 |
| 20 | 0.031 – 0.035 | 0.035 |
| 19 | 0.038 – 0.042 | 0.042 |
| 18 | 0.044 – 0.049 | 0.049 |
| 17 | 0.053 – 0.058 | 0.058 |
| 16 | 0.060 – 0.065 | 0.065 |
| 15 | 0.066 – 0.074 | 0.072 |
| 14 | 0.075 – 0.085 | 0.083 |
| 13 | 0.087 – 0.097 | 0.095 |
| 12 | 0.101 – 0.111 | 0.109 |
| 11 | 0.112 – 0.122 | 0.12 |
| 10 | 0.126 – 0.136 | 0.134 |
| 9 | 0.140 – 0.150 | 0.148 |
| 8 | 0.157 – 0.167 | 0.165 |
| 7 | 0.175 – 0.185 | 0.18 |
Chèf718 epesè kalib kare kare
| Aparèy mesi | Ranje epesè (pous) | Valè tipik (pous) |
|---|---|---|
| 22 | 0.025 – 0.029 | 0.028 |
| 20 | 0.031 – 0.035 | 0.035 |
| 19 | 0.038 – 0.042 | 0.042 |
| 18 | 0.044 – 0.049 | 0.049 |
| 17 | 0.053 – 0.058 | 0.058 |
| 16 | 0.060 – 0.065 | 0.065 |
| 15 | 0.066 – 0.074 | 0.072 |
| 14 | 0.075 – 0.085 | 0.083 |
| 13 | 0.087 – 0.097 | 0.095 |
| 12 | 0.101 – 0.111 | 0.109 |
| 11 | 0.112 – 0.122 | 0.12 |
| 10 | 0.126 – 0.136 | 0.134 |
| 9 | 0.140 – 0.150 | 0.148 |
| 8 | 0.157 – 0.167 | 0.165 |
| 7 | 0.175 – 0.185 | 0.18 |
Anviwònman GNEE Faktori Gwoup
Gnee Group Nikèl Anviwònman faktori

Gnee Gwoup Alloy 718 Tub anbalaj
Gnee Group 718 Alloy Anbalaj Tib Rektangilè

Gnee Group Inconel 718 Tès Tib Rektangilè
Gnee Group Inconel 718 Tès Tib kare

FAQ
K. Kijan ou kontwole kalite?
A: Se sètifikasyon tès moulen apwovizyone ak chajman, enspeksyon twazyèm pati ki disponib. E nou jwenn tou ISO, SGS verifye.
K: Èske ou ka fè aranjman pou chajman an?
A: Asire w, nou gen komisè machandiz pèmanan ki moun ki ka jwenn pi bon pri a soti nan pi konpayi bato epi yo ofri sèvis pwofesyonèl.
K. Ki pwodwi prensipal konpayi ou an?
A: pwodwi prensipal nou yo se asye pur, asye kabòn, asye galvanised, pwodwi aliminyòm, elatriye.
Baj popilè: Inconel 718 Tib rektangilè, Lachin Inconel 718 Swèd Tib Rektangilè