Inconel 600 fèy
Gnee Group ofri nikèl alyaj Inconel 600 nan yon varyete de fòm, ki gen ladan:
Ba
Fil
Dra
Minè
Tib
Balans
Tiyo san pwoblèm ak soude
Baton soude
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Inconel 600 Fèy prezante
600 inconel poli frèt trase manifakti plak, inconel 600 karo plak, inconel alyaj 600 shim, 600 alyaj plat plat, inconel 600 cho plak woule, inconel alyaj 600 plak founisè mondyal
Nan GNEE Group, nou devlope epi kenbe bon jan kalite ak inovasyon nan efò unremitting ak kontwòl kalite ak chanèl yo nan pwodwi nou yo. Nou ofri kliyan nou yo yon dosye bon jan kalite nan pwodwi ki ede yo chwazi pwodwi yo dwa pou endistri yo. Nou se yon ISO 9001: 2015 konpayi sètifye angaje nan bati ak jere yon biznis kliyan-santre.
Nou se manifaktirè, ajan, distribitè, founisè ak ekspòtatè nan plak inconel 600 ki se korozyon ak tanperati plak rezistan ak weldability fleksib nan tanperati diferan. UNS N06600 nou an Inconel 600 plak gen nikèl ak CHROMIUM ki fè li kapab travay nan tanperati ki ba ak fò ak dirab.
Inconel 600 fèy


Inconel 600 (Alloy 600, UNS N06600) Plak/Fèy Deskripsyon:
Inconel Alloy se yon fanmi nan superalloys nikèl-chromium ak yon trademark nan Kòporasyon Metals espesyal. Li se tipikman itilize nan aplikasyon pou gwo tanperati. Inconel Alloy 600 (UNS N06600) se souvan itilize pou aplikasyon pou ki mande pou rezistans nan korozyon ak chalè.
Inconel Alloy 600 (UNS N06600) se yon alyaj nikèl-chromium-fè ak bon rezistans oksidasyon nan tanperati ki wo ak rezistans nan klori-ion estrès korozyon fann korozyon pa dlo-wo-dlo, ak korozyon mordan.
Lòt non komès: Alloy 600, UNS N06600, W.NR 2.4816, AWS 010, Nikèl 600, Nickelvac 600, Ferrochronin 600
Inconel 600 (Alloy 600, UNS N06600) Plak/Fèy Specification:
Kalite metal: UNS N06600
Creole: ASTM B168 AMS 5540 DIN 17750
Konpozisyon chimik, %
| C | Cr | CU | Fe | Mg | NI | S | Si | |
| Max | 0.15 | 17 | 0.5 | 10 | 1 | 0.015 | 0.5 | |
| Min | 14 | 6 | 72 |
Inconel 600 fèy, lis stock plak
| Alloy 600 (75 Ni/16 cr) | Dimansyon |
|---|---|
| Dezabiye; Fwad woule, rkwit | {{0}}. 10x150 mm x bobin, 0.12 kg/m |
| Dezabiye; Fwad woule, rkwit | {{0}}. 40x200 mm x bobin, 0.7 kg/m |
| Fèy; Fwad woule, rkwit | 0. 4x914.4 mm x bobin, 3.03 kg/m |
| Fèy; Fwad woule, rkwit | 0. 5x1000 mm x bobin, 4.14 kg/m |
| Fèy; Fwad woule, rkwit | 0. 7x1000x2000 mm, 13.25 kg/pc |
| Fèy; Fwad woule, rkwit | 0. 8x1219 mm x bobin, 8.1 kg/m |
| Fèy; Fwad woule, rkwit | 1. 0 x1220 mm x bobin, 10.10 kg/m |
| Fèy; Fwad woule, rkwit | 1.2x1200x3000 mm, 37.8 kg/PC |
| Fèy; Fwad woule, marinated, rkwit | 1.6x1220x3600 mm, 59 kg/PC |
| Fèy; Fwad woule, rkwit | 2. 0 x1200x3000 mm, 62 kg/pc |
| Fèy; frèt woule, rkwit, marinated | 2.5x1200x3000 mm, 76 kg/PC |
| Fwad woule, mou rkwit, descaled, taye lenn, plak kraze, plak korektè | 3. 0 x1220x3000 mm, 92 kg/pc |
| Plak; cho woule, rkwit | 4. 0 x1200x3000 mm, 122 kg/pc |
| Plak; cho woule, rkwit | 5. 0 x2400x6000 mm, 606 kg/pc |
| Plak; cho woule, mou rkwit | 6. 0 x2440x6000 mm, 746 kg/pc |
| Plak; cho woule, descaled, rkwit | 8. 0 x2000x4000 mm, 564 kg/PCE |
| Plak; cho woule, mou rkwit | 1 0. 0x2000x4000 mm, 726 kg/pc |
| Plak; cho woule, mou rkwit | 12. 0 x2000x3000 mm, 616 kg/pc |
| Plak; cho woule, rkwit | 2 0. 0x915x1235 mm, 193 kg/pc |
ASTM B168 UNS N06600 Epesè Fèy
| Gwosè (pous) | Gwosè (mm) |
|---|---|
| .125" | 3.18mm |
| .134" | 3.40mm |
| .156" | 3.96mm |
| .187" | 4.75mm |
| .250" | 6.35mm |
| .312" | 7.92mm |
| .375" | 9.53mm |
| .500" | 12.7mm |
| .625" | 15.9mm |
| .750" | 19.1mm |
| .875" | 22.2mm |
| 1" | 25.4mm |
| 1.125" | 28.6mm |
| 1.250" | 31.8mm |
| 1.500" | 38.1mm |
| 1.750" | 44.5mm |
| 2" | 50.8mm |
| 2.500" | 63.5mm |
| 3" | 76.2mm |
Inconel alyajTès Fèy
Plak polisaj inconel

GNEE Gwoup Faktori Anviwònman
Inconel frèt fèy woule

FAQ
K: Ki jan ou kontwole bon jan kalite?
A: Se sètifikasyon tès moulen apwovizyone ak chajman, enspeksyon twazyèm pati ki disponib. E nou jwenn tou ISO, SGS, Alibaba verifye.
K: Ki avantaj ki genyen nan konpayi ou a?
A: Nou gen anpil pwofesyonèl, pèsonèl teknik, pri plis konpetitif ak pi bon sèvis apre-Dales pase lòt konpayi asye pur.
K: Konbyen coutries ou deja ekspòte?
A: Ekspòte nan plis pase 50 peyi sitou nan Amerik, Larisi, UK, Kowet, peyi Lejip, Latiki, lòt bò larivyè Jouden, peyi Zend, elatriye.
Baj popilè: Inconel 600 Fèy, Lachin Inconel 600 Fèy Swèd
Ou ka renmen tou
Voye rechèch