UNS N08810 Incoloy 800h Tib Precision
Klas: 800h
Kalite: tiyo asye san pwoblèm
Figi fen: fen tranchan, fen plat
Kòm yon founisè dirijan ak manifakti nan Lachin, GNEE Steel bay pri -efikas nikèl-pwodwi alyaj ki baze sou.
- Voye imèl -:ss@gneesteel.com
- Tel:+8615824687445
Incoloy 800h tib presizyon prezante
UNS N08810 Incoloy 800h Tib


Incoloy 800H is an iron-nickel-chromium alloy with the same basic composition as Incoloy 800, but with significantly improved creep rupture strength. The higher strength results from the tight control of the carbon, aluminum and titanium content, and the high temperature annealing process. The improvements to 800H were aimed at controlling the carbon content (0.05% to 0.10%) and grain size (>ASTM 5) Pou optimize pwopriyete kraze estrès. Incoloy 8 0 0h te plis amelyore ak yon Titàn konbine ak kontni aliminyòm (0.85% a 1.2%) asire pi bon pèfòmans tanperati ki wo. Alloy a se doub sètifye, konbine pèfòmans nan tou de fòm yo.
Incoloy 800h tib se yon tanperati ki wo nikèl-fè-Chromium alyaj ak ranfòse rezistans fluaj ak ekselan estabilite nan aplikasyon pou tanperati ki wo, fè li ideyal pou ekipman tretman chalè ak pwosesis petrochimik. Steel Gnee se yon founisè nan alyaj ki baze sou nikèl. Nou kounye a ofri Incoloy 800H (UNS N08810) tib nan diferan gwosè nan pri trè konpetitif.
Incoloy 800h espesifikasyon tiyo san pwoblèm
| Estanda | : | ASTM / ASME |
| Deziyasyon | : | ASTM B 407/ ASME SB 407 |
| Tay | : | 4 a 219mm wt: 0. 5 a 20mm |
| Klas | : | Incoloy 800H (UNS N08810) san pwoblèm PIPES1.4958 |
| Longè | : | Nan 13500mm |
| Lèt | : | San pwoblèm |
| Fòm | : | Wonn, kare, rektangilè, idwolik elatriye. |
800h incoloy tiyo san pwoblèm ekivalan klas
| Estanda | Ògje | WERKSTOFF NR. | Afnor | En | JIS | BS | GOST | Ou |
| Incoloy 800h | N08810 | 1.4958 | Z8NC 32-21 | X10Nicralti 32-20 | NCF 800H | Na 15 (h) | ЭИ670 | XH32T |
Incoloy UNS N08810 Tiyo san pwoblèm konpozisyon chimik
| Egalize | NI | C | Fe | Si | Mn | S | Al | Ti | CU | Cr |
| Incoloy 800h | 30-35 | 0.05-0.1 | 39.5 min | 1. 0 max | 1.5 Max | 0. 015 Max | 0.15-0.60 | 0.15-0.60 | 0. 75 Max | 19-23 |
Gnee Gwoup Product anbalaj
Uns n 08810 800 h tib presizyon

Anviwònman GNEE Faktori Gwoup
Incoloy 800h tib

FAQ
K: Ki avantaj ki genyen nan konpayi ou a?
A: Nou gen anpil pwofesyonèl, teknisyen, pri plis konpetitif ak pi bon sèvis la apre-lavant pase lòt konpayi asye pur.
K: Konbyen peyi ou ekspòte?
A: Ekspòte nan plis pase 50 peyi, sitou nan Etazini yo, Larisi, Wayòm Ini a, Kowet, peyi Lejip, Latiki, lòt bò larivyè Jouden, peyi Zend, elatriye.
K: Èske ou ka bay echantiyon yo?
Repons: Wi. Osi lontan ke ou kontakte nou, nou ka bay echantiyon gratis ti nan stock. Echantiyon Customized pral pran sou 5-7 jou.